Critical slowing of the spin and charge density wave order in thin film Cr following photoexcitation
Sheena K. K. Patel, Oleg Yu. Gorobtsov, Devin Cela, Stjepan B. Hrkac, Nelson Hua, Rajasekhar Medapalli, Anatoly G. Shabalin, James Wingert, James M. Glownia, Di… 展开作者
Sheena K. K. Patel, Oleg Yu. Gorobtsov, Devin Cela, Stjepan B. Hrkac, Nelson Hua, Rajasekhar Medapalli, Anatoly G. Shabalin, James Wingert, James M. Glownia, Diling Zhu, Matthieu Chollet, Oleg G. Shpyrko, Andrej Singer, Eric E. Fullerton
我们报道了铬薄膜在超快光学激光脉冲光激发后,其电荷密度波(charge density wave, CDW)和自旋密度波(spin density wave, SDW)有序的演化过程。通过对CDW卫星峰的超快时间分辨X射线衍射测量CDW,追踪光激发后CDW的抑制与恢复过程。我们发现,当薄膜温度接近CDW和SDW有序的不连续相变时,恢复时间尺度相较于预期的热时间尺度呈指数增长。我们扩展了适用于SDW系统的Landau模型,结合薄膜系统几何结构施加的合适边界条件,以解释这种临界减慢现象。该模型使我们能够评估具有不同空间周期性的可用CDW/SDW态之间的能垒。
英文摘要:
We report on the evolution of the charge density wave (CDW) and spin density wave (SDW) order of a chromium film following photoexcitation with an ultrafast optical laser pulse. The CDW is measured by ultrafast time-resolved x-ray diffraction of the CDW satellite that tracks the suppression and recovery of the CDW following photoexcitation. We find that as the temperature of the film approaches a discontinuous phase transition in the CDW and SDW order, the time scales of recovery increase exponentially from the expected thermal time scales. We extend a Landau model for SDW systems to account for this critical slowing with the appropriate boundary conditions imposed by the geometry of the thin film system. This model allows us to assess the energy barrier between available CDW/SDW states with different spatial periodicities.
Air-Water Interface-Assisted Synthesis and Charge Transport Characterization of Quasi-2D Polyacetylene Films with Enhanced Electron Mobility via Ring-Opening Polymerization of Pyrrole
Exploring the structural , electronic and magnetic properties of cation ordered 3d-5d double perovskite Bi$_2$FeReO$_6$ and Bi$_2$FeIrO$_6$ thin-films from first-principles
Coherent dynamics of mixed Frenkel and Charge Transfer Excitons in Dinaphtho[2,3-b:2'3'-f]thieno[3,2-b]-thiophene Thin Films: The Importance of Hole Delocalization
Higher critical currents yet faster vortex creep in EuBa$_2$Cu$_3$O$_y$ films containing coherent artificial pinning centers
University of Washington(华盛顿大学);Seikei University(圣心女子大学);Japan Fine Ceramics Center(日本精细陶瓷中心);National Institute of Advanced Industrial Science and Technology(产业技术综合研究所)