Mg-Mn-Al-O薄膜体系相组成的高通量研究及其与从渣中回收锂的关系
High-throughput study of the phase constitution of the thin film system Mg-Mn-Al-O in relation to Li recovery from slags
AI总结:
本文利用薄膜材料库和高通量表征方法系统研究了Mg-Mn-Al-O渣子体系的相组成,证实了宽广成分范围内尖晶石固溶体的形成,并揭示Mn氧化态控制对促进锂回收所需EnAM相形成的潜在作用。
摘要:
回收利用的重要性日益增加,使得从渣中回收有价元素变得引人关注,例如通过工程人工矿物(EnAMs)的概念。在该概念中,目标是从火法冶金回收过程的渣中形成EnAMs,即具有高含量待回收元素的相。为此,理解渣体系的相组成具有很高的重要性。Mg-Mn-Al-O体系是锂离子电池回收中的一个金属氧化物渣子体系,对尖晶石相的形成至关重要,而尖晶石相是与可能含锂的EnAM相LiAlO2竞争的相。本文利用覆盖成分空间(Mg14-69Mn11-38Al14-74)Ox的薄膜材料库研究了相组成。通过高通量能量色散X射线光谱和X射线衍射,证实了尖晶石固溶体相在宽广成分空间内的形成。发现随着Mg含量的增加,尖晶石固溶体沿(400)方向的择优取向增强。利用X射线光电子能谱测量了材料库选定区域的近表面成分,对Mn 2p3/2区域的详细峰拟合揭示Mn的氧化态为Mn2+和Mn3+的混合物。对于材料库中一个含有等原子量Mg、Mn和Al的测量区域,透射电子显微镜显示,约420 nm厚的薄膜由柱状尖晶石晶粒组成,Mg、Mn和Al均匀分布。基于这些结果,我们认为,所展示的渣中尖晶石形成的高可能性可能通过控制Mn氧化态来加以影响,从而促进所需EnAM相的形成。
英文摘要:
The increasing importance of recycling makes the recovery of valuable elements from slags interesting, e.g., by the concept of engineered artificial minerals (EnAMs). In this concept, it is aimed for the formation of EnAMs, meaning phase(s) with a high content of the to-be-recovered element(s) from slags of pyrometallurgical recycling processes. For this, understanding the phase constitution of the slag systems is of high importance. The system Mg-Mn-Al-O is a metal oxide slag subsystem from Li-ion battery recycling, that is critical for the formation of spinel phases, which are competing phases to the possible Li-containing EnAM phase LiAlO2. Here, the phase constitution was investigated using a thin film materials library that covers the composition space (Mg14-69Mn11-38Al14-74)Ox. By means of high-throughput energy-dispersive X-ray spectroscopy and X-ray diffraction, the formation of the spinel solid solution phase was confirmed for a wide composition space. Increasing preferential orientation of the spinel solid solution along (400) with increasing Mg content was identified. X-ray photoelectron spectroscopy was used to measure the near-surface composition of selected areas of the materials library, and detailed peak fitting of the Mn 2p3/2 region revealed the Mn oxidation state to be a mixture of Mn2+ and Mn3+. For one measurement area of the materials library containing equal atomic amounts of Mg, Mn and Al, transmission electron microscopy showed that the approximately 420 nm-thick film consists of columnar spinel grains with Mg, Mn and Al being evenly distributed. Based on these results, we suggest that the shown high likelihood of spinel formation in slags might be influenced by controlling the Mn oxidation state to enable the formation of desirable EnAM phases.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。