arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2311.04021physics.ins-dethep-ex
收藏

一种用于超导磁体浸渍的新型高延展性、高韧性树脂

A New Ductile, Tougher Resin for Impregnation of Superconducting Magnets

Emanuela Barzi, Daniele Turrioni, Ibrahim Kesgin, Masaki Takeuchi, Wang Xudong, Tatsushi Nakamoto, Akihiro Kikuchi

AI总结:

本研究针对Nb3Sn高场磁体的训练效应问题,采用新型TELENE树脂浸渍磁体大幅减少失超次数,还通过混合高比热容陶瓷粉末提升其比热容并测试辐照性能,有望降低加速器调试成本。

摘要:

$Nb_3Sn$高场磁体面临的一个主要遗留挑战是线圈中随机温度变化导致的训练效应。本研究的主要目标是找到相对于当前使用的环氧树脂的新型浸渍材料,以减少或消除这种训练效应。我们采用了一种有机烯烃基热固性二环戊二烯(DCP)树脂$C_10H_{12}$(日本RIMTEC公司的市售产品TELENE),对由ANL和FNAL开发的短$Nb_3Sn$波荡器线圈进行浸渍。该磁体仅经历两次失超后就达到了短样极限,而使用CTD-101K时则需要数十次失超。研究证实,延展性(即承受大应变的能力)和韧性是实现这一结果的关键性能。此外,我们还研究了将TELENE与高比热容陶瓷粉末混合是否能提高浸渍后$Nb_3Sn$超导磁体的比热容($C_p$)。本研究测量了添加高$C_p$粉末填料的TELENE的黏度、比热容、热导率及其他物理性能随温度和磁场的变化关系。将TELENE与$Gd_2O_3$、$Gd_2O_2S$或$HoCu_2$混合后,其比热容提升了10倍。我们还在日本高崎的高崎先进辐射研究所,研究了10戈瑞伽马射线辐照对纯TELENE及混合TELENE力学性能的影响。尽管TELENE-82wt%$Gd_2O_3$和TELENE-83wt%$HoCu_2$均表现良好,但辐照后力学性能最佳的是TELENE-87wt%$Gd_2O_2S$。未来将使用后一种浸渍材料对短波荡器进行测试,以验证其是否能进一步提升线圈的热稳定性。更短的磁体训练周期将提升磁体可靠性、降低风险,并大幅节省加速器的调试成本。

英文摘要:

A major remaining challenge for $Nb_3Sn$ high field magnets is their training due to random temperature variations in the coils. The main objective of our research is to reduce or eliminate it by finding novel impregnation materials with respect to the epoxies currently used. An organic olefin-based thermosetting dicyclopentadiene (DCP) resin, $C_10H_12$, commercially available in Japan as TELENE by RIMTEC, was used to impregnate a short $Nb_3Sn$ undulator coil developed by ANL and FNAL. This magnet reached short sample limit after only two quenches, compared with several dozens when $CTD-101K$ was used. Ductility, i.e. the ability to accept large strains, and toughness were identified as key properties to achieve these results. In addition, we have been investigating whether mixing TELENE with high heat capacity ceramic powders, increases the specific heat ($C_p$) of impregnated $Nb_3Sn$ superconducting magnets. The viscosity, heat capacity, thermal conductivity, and other physical properties of TELENE with $high-C_p$ powder fillers were measured in this study as a function of temperature and magnetic field. Mixing TELENE with either $Gd_2O_3$, $Gd_2O_2S$, and $HoCu_2$ increases its $C_p$ tenfold. We have also investigated the effect on the mechanical properties of pure and mixed TELENE under 10 $Gy$ of gamma-ray irradiation at the Takasaki Advanced Radiation Research Institute in Takasaki, Japan. Whereas both $TELENE-82wt\%Gd_2O_3$ and $TELENE-83wt\%HoCu_2$ performed well, the best mechanical properties after irradiation were obtained for $TELENE-87wt\%Gd2O_2S$. Testing a short undulator in the future with the latter impregnation material will verify whether it will further improve the coils thermal stability. Short magnet training will lead to better magnet reliability, lower risk and substantial saving in accelerators commissioning costs.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑