高温下铌取代镧基正钒酸盐的介电行为与阻抗谱
Dielectric behavior and impedance spectroscopy of Niobium substituted Lanthanum based orthovanadates at high temperatures
AI总结:
本研究系统探究了不同铌取代量的镧基正钒酸盐LaV$_{1-x}$Nb$_x$O$_4$的高温介电与阻抗特性,揭示了晶体结构与介电行为的关联,明确了各组分的弛豫活化能与电导机制。
摘要:
我们对通过固相反应法制备的LaV$_{1-x}$Nb$_x$O$_4$($x=$ 0-1)样品的温度依赖介电特性、阻抗谱及电导率开展了详细研究。介电常数($ε_r'$)随温度升高而增大、随频率升高而减小;同时$ε_r'$的幅值随$x$基本保持不变(在100 Hz、600℃条件下约为10$^4$量级)。单相的$x=$ 0(单斜独居石结构,$P2_1/n$)与$x =$ 1(单斜褐钇铌矿结构,$I2/a$)样品的损耗因子[tan$δ=$ (4-8)]低于具有四方与单斜混合相的$x=$ 0-0.8样品[tan$δ=$(12-18)],这表明晶体结构与介电特性之间存在强关联。阻抗的实部随温度和频率升高均减小,观测到的弱弛豫现象随$x$变化基本保持不变。阻抗的虚部呈现出强弛豫峰,且弛豫峰随频率升高向更高温度偏移,这归因于样品中晶粒、晶界与电极的作用。弛豫过程的活化能经估算:$x=$ 0-0.6的样品为0.8-1.0 eV,$x=$ 0.8的样品约为1.4 eV;而$x=$ 1的样品在高温区和低温区分别呈现两个活化能值(约0.5 eV和约1.0 eV)。此外,总电导率随角频率的变化(范围在10$^{-3}$至10$^{-5}$ S/m之间)采用Jonsher幂律进行拟合。分析表明所有样品均符合OLPT(重叠大极化子隧穿)模型,而$x$ = 1的样品在480℃附近存在相变,在更高温度下表现出NSPT(近程小极化子隧穿)和QMT(量子力学隧穿)行为。该相变得到了正切损耗曲线的佐证,且可能与结构变化相关。
英文摘要:
We present the detailed study of the temperature dependent dielectric properties, impedance spectroscopy and electrical conductivity of LaV$_{1-x}$Nb$_x$O$_4$ ($x=$ 0-1) samples prepared by the solid-state reaction method. The dielectric constant ($ε_r'$) increases (decreases) with increase in the temperature (frequency); while, the magnitude of $ε_r'$ remains almost invariant (order of 10$^4$ at 100~Hz and 600\degree C) with $x$. The single phase $x=$ 0 (monoclinic-monazite, $P2_1/n$) and $x =$ 1 (monoclinic fergusonite, $I2/a$) samples show the lower values of loss factor [tan$δ=$ (4-8)] as compared to the $x=$ 0-0.8 samples [tan$δ=$(12-18)] having mixed tetragonal and monoclinic phases, which indicates the strong correlation between the crystal structure and the dielectric properties. The real part of impedance decreases with both temperature and frequency, and the observed weak relaxation remains almost unaltered with $x$. The imaginary part of impedance shows strong relaxation peaks shifting towards higher temperatures with frequency, which is attributed to the effect of grains, grain boundaries, and electrodes in the samples. The activation energy of the relaxation process is estimated to be 0.8-1.0~eV for the $x=$ 0-0.6 samples, and $\approx$1.4~eV for the $x=$ 0.8; whereas the $x=$ 1 sample shows two values ($\approx$0.5~eV and $\approx$1.0~eV) in the higher and lower temperature range, respectively. Further, the change in total conductivity with the angular frequency, which found to be in the range of 10$^{-3}$ to 10$^{-5}$~S/m, is fitted using the Jonsher power law. The analysis suggests the OLPT model for all the samples, whereas the $x$ = 1 sample exhibit a transition near 480\degree C and at higher temperatures it shows NSPT and QMT. This transition is corroborated by the tangent loss curves and may be associated with the change in structure.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。