Ti-6Al-4V在微动下摩擦学转变结构(TTS)的异质性
Heterogeneity in tribologically transformed structure (TTS) of Ti-6Al-4V under fretting
AI总结:
本文研究了Ti-6Al-4V合金在微动下摩擦学转变结构(TTS)的形成,发现TTS的出现取决于接触压力和循环次数,并利用FIB和TEM揭示了其由两个交替的纳米晶粒区域组成的异质微观结构。
摘要:
微动磨损是由振荡运动和接触滑动引起的表面退化过程。在完全滑移阶段,表面和次表面的高局部应力与塑性变形会导致一种称为摩擦学转变结构(TTS)的纳米晶粒结构的形成。本文研究了在微动载荷下改变接触压力和微动循环次数时,TTS在α-β型Ti-6Al-4V合金中的形成过程。磨损疤痕的横截面在抛光和化学蚀刻后进行观察。当压力高于300 MPa的阈值时,TTS在接触早期(1000次循环之前)出现,同时伴随另外两种结构:由压实磨屑组成的第三体层(TBL)和位于TTS下方的塑性区即一般变形层(GDL)。TTS最初以岛屿状出现,在足够多的循环后于接触中心融合。低于200 MPa时,仅形成TBL和GDL。在200 MPa时,仅发现小范围的局部TTS。除氮化的TBL外,所有结构的化学成分均与初始基体材料相同。与基体相比,TTS具有极高的硬度。使用聚焦离子束(FIB)小心提取了TTS,并用透射电子显微镜(TEM)观察其微观结构。结果显示出极端的晶粒细化,并由两个交替区域组成。第一个区域I由尺寸为20至50 nm且具有结晶织构的α晶粒组成。区域II包含尺寸为5至20 nm且无织构的纳米等轴晶粒。研究结果使得建立根据接触压力和微动循环次数条件下的TTS出现情景成为可能。
英文摘要:
Fretting wear is a surface degradation process caused by oscillatory motion and contact slipping. During gross slip, high local stresses and plastic deformation in the surface and subsurface can lead to the creation of a nanosized grained structure called Tribologically Transformed Structure (TTS). The current paper studies the formation of TTS in an alpha-beta Ti-6Al-4V alloy under fretting loading while changing the contact pressure and the number of fretting cycles.Cross-sections of wear scars are observed after polishing and chemical etching. Above a threshold pressure of 300 MPa, TTS appears early in the contact (before 1000 cycles) along with two other structures: a Third Body Layer (TBL) made of compacted debris and a General Deformed Layer (GDL) which is the plastic zone under the TTS. TTS first appears as islands and merges in the middle of the contact after enough cycles. Below 200 MPa, only TBL and GDL are formed. At 200 MPa, only small, localized TTS is found. All structures have the same chemical compositions as the initial bulk material except for the nitrided TBL. TTS has a very high hardness compared to the bulk. TTS was carefully extracted using a Focused Ion Beam (FIB) and its microstructure was observed with a Transmission Electron Microscope (TEM). It shows extreme grain refinement and is composed of two alternated zones. The first zone I is composed of $α$ grains with a size of 20 to 50 nm with crystallographic texture. Zone II comprises nanosized equiaxed grains whose sizes range from 5 to 20 nm without texture. The results made it possible to establish a scenario of the appearance of the TTS according to the conditions of contact pressure and number of fretting cycles.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。