arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2310.12416cond-mat.mtrl-sci
收藏

粉末床熔融-激光束制备的氧化物弥散强化合金中弥散体尺寸与数密度的极限

Limits of dispersoid size and number density in oxide dispersion strengthened alloys fabricated with powder bed fusion-laser beam

Nathan A. Wassermann, Yongchang Li, Alexander J. Myers, Christopher A. Kantzos, Timothy M. Smith, Jack L. Beuth, Jonathan A. Malen, Lin Shao, Alan J. H. McGaughey, Sneha P. Narra

AI总结:

本研究结合实验与热力学动力学建模,探究粉末床熔融-激光束制备氧化物弥散强化合金中弥散体尺寸和数密度的极限,发现碰撞粗化是限制因素,并提出优化加工策略。

摘要:

先前关于增材制造氧化物弥散强化合金的研究主要采用实验方法,所得弥散体尺寸大于传统粉末冶金所能达到的水平,而数密度则更低。为改善制备态微观组织,本研究将实验与热力学和动力学建模框架相结合,探究粉末床熔融-激光束工艺所能实现的弥散体尺寸与数密度的极限。采用一系列激光功率和扫描速度组合制备了Ni-20Cr+1 wt.% Y2O3合金块体样品。利用扫描透射电子显微镜表征量化了加工参数空间内的弥散体尺寸分布。在300 W和1200 mm/s条件下观察到最小平均弥散体直径(29 nm),数密度为1.0×10^20 m^-3;在200 W和200 mm/s条件下观察到最大平均直径(72 nm),数密度为1.5×10^19 m^-3。扫描电子显微镜结果表明,由于氧化物团聚以及富含氧化物的飞溅从熔池中喷出,添加到原料中的氧化物有相当一部分在加工过程中损失。在考虑这些损失后,模型对弥散体直径和数密度的预测与实验趋势一致。结果表明,限制最终数密度的机制是熔池中弥散体的碰撞粗化。利用该建模框架提出了限制弥散体尺寸并提高数密度的加工策略。

英文摘要:

Previous work on additively-manufactured oxide dispersion strengthened alloys focused on experimental approaches, resulting in larger dispersoid sizes and lower number densities than can be achieved with conventional powder metallurgy. To improve the as-fabricated microstructure, this work integrates experiments with a thermodynamic and kinetic modeling framework to probe the limits of the dispersoid sizes and number densities that can be achieved with powder bed fusion-laser beam. Bulk samples of a Ni-20Cr $+$ 1 wt.% Y$_2$O$_3$ alloy are fabricated using a range of laser power and scanning velocity combinations. Scanning transmission electron microscopy characterization is performed to quantify the dispersoid size distributions across the processing space. The smallest mean dispersoid diameter (29 nm) is observed at 300 W and 1200 mm/s, with a number density of 1.0$\times$10$^{20}$ m$^{-3}$. The largest mean diameter (72 nm) is observed at 200 W and 200 mm/s, with a number density of 1.5$\times$10$^{19}$ m$^{-3}$. Scanning electron microscopy suggests that a considerable fraction of the oxide added to the feedstock is lost during processing, due to oxide agglomeration and the ejection of oxide-rich spatter from the melt pool. After accounting for these losses, the model predictions for the dispersoid diameter and number density align with the experimental trends. The results suggest that the mechanism that limits the final number density is collision coarsening of dispersoids in the melt pool. The modeling framework is leveraged to propose processing strategies to limit dispersoid size and increase number density.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑