arXivDaily arXiv每日学术速递 周一至周五更新
arXiv周末暂无论文更新,休息一下吧,周末愉快~~
arXiv 2310.01752physics.app-ph
收藏

Piezo-to-Piezo (P2P) 转换:通过MHz量级纳米机电振动实现超薄、透明且自支撑的均聚物PVDF薄膜的β相结晶与极化同步进行

Piezo-to-Piezo (P2P) Conversion: Simultaneous $β$-Phase Crystallization and Poling of Ultrathin, Transparent and Freestanding Homopolymer PVDF Films via MHz-Order Nanoelectromechanical Vibration

Robert Komljenovic, Peter C. Sherrell, Amgad R. Rezk, Leslie Y. Yeo

AI总结:

本研究提出P2P转换的低能耗新方法,利用MHz级纳米机电振动同步实现PVDF薄膜的β相结晶与极化,制备出的自支撑透明纯PVDF薄膜压电性能优于商用同类产品,适用于能量收集领域。

摘要:

本文报道了一种非常规但简便的低能耗方法,该方法通过压电-压电(P2P)转换独特合成纯聚偏氟乙烯(PVDF)薄膜,用于能量收集应用。在这一全新概念中,压电衬底产生的纳米机电能量在另一可极化材料(即PVDF)结晶过程中被直接耦合到该材料中,制备出微米级厚度的薄膜。该薄膜不仅表现出强压电性,还具备自支撑性和光学透明性——这些特性是能量收集应用的理想选择,但通过传统合成路线难以实现。具体而言,研究表明,以表面反射体波(SRBWs)形式存在的纳米机电振动所产生的前所未有的加速度(量级为10^8 m s^-2),促进了铁电PVDF β相的择优取向成核;同时,SRBWs强烈的本征倏逝电场(量级为10^8 V m^-1)使PVDF的偶极子排列,从而实现材料极化。通过这种仅需量级为10 V低电压的方法合成的纯(无添加剂)均聚物薄膜,其电压比能耗巨大的传统高千伏电势极化方法低数个数量级。与厚度相近的金标准商业极化PVDF薄膜相比,该薄膜的宏观压电电荷系数(d33)高出76%,发电输出也有类似提升。

英文摘要:

An unconventional yet facile low-energy method for uniquely synthesizing neat poly(vinylidene fluoride) (PVDF) films for energy harvesting applications through piezo-to-piezo (P2P) conversion is reported. In this novel concept, the nanoelectromechanical energy from a piezoelectric substrate is directly coupled into another polarizable material (i.e., PVDF) during its crystallization to produce a micron-thick film that not only exhibits strong piezoelectricity, but is also freestanding and optically transparent - properties ideal for its use for energy harvesting, but which are difficult to achieve through conventional synthesis routes. In particular, we show that the unprecedented acceleration ($\mathcal{O}$($10^{8}$ m s$^{-2}$)) associated with the nanoelectromechanical vibration in the form of surface reflected bulk waves (SRBWs) facilitates preferentially-oriented nucleation of the ferroelectric PVDF $β$-phase, while simultaneously aligning its dipoles to pole the material through the SRBW's intense native evanescent electric field ($\mathcal{O}$($10^{8}$ V m$^{-1}$)). The resultant neat (additive-free) homopolymer film synthesized through this low voltage method requiring only $\mathcal{O}$(10 V) - orders-of-magnitude lower than the energy-intensive conventional poling methods utilising high kV electric potentials - is shown to possess a 76% higher macroscale piezoelectric charge coefficient ($d_{33}$), together with a similar improvement in its power generation output, when compared to the gold-standard commercially-poled PVDF films of similar thicknesses.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑