阳离子空位浓度对$(1-x)$BiVO$_4$-$x$Bi$_{2/3}$MoO$_4$白钨矿固溶体超低热导率的影响
Influence of cation vacancy concentrations on ultra-low thermal conductivity in $(1-x)$BiVO$_4$-$x$Bi$_{2/3}$MoO$_4$ scheelite solid solutions
AI总结:
通过制备钒酸铋-钼酸铋固溶体陶瓷,发现仅添加极少量的阳离子空位即可使热导率大幅降低15%以上,同时保持高温稳定性,是制备热障和热电器件优质材料的最佳策略。
摘要:
制备了钒酸铋-钼酸铋固溶体,以详细研究具有不同阳离子空位含量的陶瓷。获得了微观结构相似的致密陶瓷,并评估了其熔点、比热、热扩散率和热导率随空位量变化的演变。在室温下,热导率从BiVO$_4$(x=0)的1.74 W m$^{-1}$ K$^{-1}$降至Bi$_{0.867}$$\square$$_{0.133}$Mo$_{0.4}$V$_{0.6}$O$_4$(x=0.4)的1.12 W m$^{-1}$ K$^{-1}$。此外,我们表明极少量的空位(1.7%,x=0.05)就足以使热导率大幅降低15%以上,这与质量涨落散射模型一致。然而,熔点温度也随空位量增加而降低。我们的结果表明,仅添加极少量的空位是获得具有超低热导率和高温稳定性的热障及热电器件优质材料的最佳策略。
英文摘要:
Bismuth vanadate - bismuth molybdate solid-solution was prepared to elaborate ceramics with different amounts of cation vacancies. Dense ceramics with similar microstructures were obtained and the evolution of their melting point, specific heat, thermal diffusivity, and conductivity as a function of the amount of vacancy was evaluated. At room temperature, the thermal conductivity decreases from 1.74 W m$^{-1}$ K$^{-1}$ for BiVO$_{4}$ (x=0) to 1.12 W m$^{-1}$ K$^{-1}$ for Bi$_{0.867}$$\square$$_{0.133}$Mo$_{0.4}$V$_{0.6}$O$_{4}$ (x=0.4). Moreover, we show that a very small amount of vacancy (1.7%, x=0.05) is enough to provide a large decrease in thermal conductivity by more than 15%, in agreement with a mass fluctuation scattering model. However, the temperature of the melting point also decreases with increasing amount of vacancy. Our results suggest adding only a very small amount of vacancy as the best strategy to obtain superior materials for thermal barriers and thermoelectric devices, with ultra-low thermal conductivity and high-temperature stability.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。