c轴蓝宝石上低损耗超导Ta薄膜的晶粒尺寸
Grain size in low loss superconducting Ta thin films on c-axis sapphire
AI总结:
针对c轴蓝宝石上α-Ta薄膜晶粒尺寸与超导器件性能关联的假说,开展对比实验,结合室温表征与低温测量发现二者无统计差异,缩小了该超导量子材料体系的优化参数空间。
摘要:
近年来,Ta薄膜的应用已提升了超导电路的相干时间,进一步优化该材料体系成为超导量子计算材料子领域的研究重点。此前有假说认为晶粒尺寸可能与器件性能相关。本研究针对c轴蓝宝石上的α-Ta开展了晶粒尺寸对比实验,评估方法涵盖室温化学与结构表征以及低温微波测量。结果显示,晶粒尺寸分别为924 nm²的小晶粒器件与1700 nm²的大晶粒器件在性能上无统计学差异。这表明在c轴蓝宝石上生长的Ta的相关参数范围内,晶粒尺寸与损耗无关联,缩小了该材料体系的优化参数空间。
英文摘要:
In recent years, the implementation of thin-film Ta has led to improved coherence times in superconducting circuits. Efforts to further optimize this materials set have become a focus of the subfield of materials for superconducting quantum computing. It has been previously hypothesized that grain size could be correlated with device performance. In this work, we perform a comparative grain size experiment with $α$-Ta on $c$-axis sapphire. Our evaluation methods include both room-temperature chemical and structural characterization and cryogenic microwave measurements, and we report no statistical difference in device performance between small- and larger-grain-size devices with grain sizes of 924 nm$^2$ and 1700 nm$^2$, respectively. These findings suggest that grain size is not correlated with loss in the parameter regime of interest for Ta grown on c-axis sapphire, narrowing the parameter space for optimization of this materials set.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。