受限条件下氢键低聚物PMMS的润湿性与平衡速率之间是否存在关系?
Is there a relationship between wettability and rates of equilibration of the H-bonded oligomer PMMS under confinement?
AI总结:
本文通过介电谱、DSC和接触角测量研究PMMS在AAO和二氧化硅纳米孔中的退火行为,发现受限诱导的弛豫偏离可通过特定温度退火消除,且平衡活化能随孔径和模板材料显著变化,并归因于润湿性变化对界面分子交换和吸附-脱附过程的影响。
摘要:
本文利用宽带介电谱(BDS),并辅以差示扫描量热法(DSC)和温度依赖的接触角θ测量,研究了聚(巯丙基甲基硅氧烷,PMMS)在两种多孔模板(阳极氧化铝,AAO,和二氧化硅)中受限时的退火实验,这两种模板具有不同的孔径,d=8-120 nm,并采用了不同的热程序(冷却/加热速率显著不同)。研究发现,由常规温度依赖介电测量得到的弛豫时间在接近玻璃化转变温度时偏离体相行为。重要的是,这种受限诱导效应可以通过在特定温度范围内进行的退火实验轻易消除。对预先以不同速率冷却的受限样品在等温实验中收集的介电数据的分析表明:(i)退火的恒定速率随冷却而变长,并且弱依赖于冷却速率;(ii)平衡过程的活化能E_a随孔径的减小以及多孔模板材料的不同而变化。事实上,在AAO(d=10 nm)和二氧化硅(d=8 nm)膜中进行的退火过程所获得的E_a显著降低,分别从约62 kJ/mol降至约23 kJ/mol。E_a的这种显著变化可以通过考虑PMMS的温度依赖θ来解释,这表明冷却时两种表面之间的润湿性发生了显著变化。因此,可以预期界面分子与核心分子之间的质量交换以及较低温度下界面处发生的吸附-脱附过程必定受到影响。
英文摘要:
In this paper, we investigated the annealing experiments of poly(mercaptopropylmethylsiloxane, PMMS) confined within two types of porous templates (anodic aluminium oxide, AAO, and silica) characterized by different pore diameter, d= 8-120nm, using different thermal protocols (varying significantly in cooling/heating rate) by means of Broadband Dielectric Spectroscopy (BDS) supported by the complementary Differential Scanning Calorimetry (DSC) and temperature-dependent contact angle, θ, measurements. It was found that relaxation times obtained from routine temperature-dependent dielectric investigations deviate from the bulk behavior when approaching the glass transition temperature. Importantly, this confinement induced effect can be easily removed by the annealing experiments performed at some specific range of temperatures. The analysis of the dielectric data collected during isothermal experiments of confined samples that was beforehand cooled with different rates revealed that (i) constant rates of annealing gets longer with cooling and weakly depend on the rate of cooling, and (ii) activation energy of the equilibration process, E_a, varies with the reduction of the pore diameter and material the porous template is made of. In fact, there is significant reduction in E_a from ~62 to ~23 kJ/mol obtained for the annealing process carried out in AAO (d= 10 nm) and silica (d= 8 nm) membranes, respectively. Such significant change in E_a can be explained taking into account temperature-dependence of θ of PMMS indicating a notable change in wettability between both surfaces upon cooling. As a consequence, one can expect that the mass exchange between interfacial and core molecules as well as adsorption-desorption processes occurring at the interface at lower temperatures must be affected.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。