结合X射线纳米CT与XANES技术对NMC电极中锂化空间组成演化的三维原位监测

In Situ Three-Dimensional Mapping of Lithiation Heterogeneity in NMC Electrodes using XANES Nanotomography

Université UPJV(皮卡第儒勒-凡尔纳大学);Renault Technocentre(雷诺技术中心);Advanced Photon Source, Argonne National Laboratory(阿贡国家实验室先进光子源)

Tuan-Tu Nguyen, Jiahui Xu, Zeliang Su, Vincent De Andrade, Alejandro A. Franco, Bruno Delobel, Charles Delacourt, Arnaud Demortière

AI总结:

本文提出结合XANES与TXM-nanoCT的三能级原位方法,在降低辐射损伤的同时实现NMC电极三维(脱)锂化追踪,揭示核壳结构与不均匀锂化,并可推广至高活性材料密度电极研究。

摘要:

在本研究中,我们提出了一种明确的方法论,用于在LiNi$_{0.5}$Mn$_{0.3}$Co$_{0.2}$O$_2$(NMC)正极电极上进行原位X射线吸收近边结构谱学(XANES)与透射X射线纳米计算机断层扫描(TXM-nanoCT)联合实验。为了在充放电循环过程中尽量减少辐射对样品造成的损伤,并获得活性材料(脱)锂化过程的全面三维视角,我们提出了一种新方法,该方法仅依赖三个能量水平,分别策略性地设置在前边、边和后边位置。通过采用该技术,我们成功地在部分循环过程中追踪了三维空间内的各种(脱)锂化状态。此外,我们还能够提取单个二次颗粒内部的纳米级锂分布。我们的观察揭示了锂化过程中核壳结构的形成,并且我们还发现并非颗粒的所有表面区域在该过程中都表现出活性。值得注意的是,锂嵌入表现出明显的偏好性,导致不同电极位置之间的锂化程度不均匀。所提出的方法不仅限于NMC正极电极,还可以扩展到研究具有高活性材料(AM)密度的真实专用电极,从而促进对此类电极内部异质性和不均匀锂化的探索与量化。这种对电极内部(脱)锂化过程及锂化异质性的多尺度洞察,有望为优化电极设计并最终在材料科学和电池材料研究背景下提升电极性能提供有价值的知识。

英文摘要:

Spatial heterogeneity in lithiation complicates the interpretation of electrode-averaged electrochemical measurements and the assessment of local active-material utilization. Here, we use three-energy X-ray absorption near-edge structure (XANES) nanotomography to investigate lithiation distributions in NMC532 composite electrodes with active-material loadings of 3 and 15 mg cm-2. Tomographic acquisitions at 8.30, 8.35, and 8.43 keV combine three-dimensional particle morphology with Ni K-edge chemical sensitivity at a processed voxel size of 210 nm. The normalized absorption contrast serves as a relative lithiation indicator, without assigning absolute lithium concentrations. Measurements were performed in situ after 1 h of open-circuit relaxation at selected electrochemical states. In the lower-loading electrode, four successive states during interrupted discharge at 2 mA cm-2 reveal an increasing lithium-rich volume fraction alongside core-shell-like distributions, nonuniform peripheral enrichment, and particle-to-particle variability. In the higher-loading electrode, two regions examined at 50% depth of discharge exhibit different lithiation-sensitive contrast distributions despite sharing the same nominal electrochemical state. These observations document heterogeneity within particles, between particles, and between electrode regions, showing how overall lithiation progression can coexist with spatially nonuniform local states. Three-energy XANES nanotomography thus provides a means of examining lithiation heterogeneity in dense composite electrodes with limited spectral sampling. Correlative phase-contrast imaging could further relate these distributions to the arrangement of the carbon-binder domain and pore network.