arXiv 2305.02698cond-mat.mtrl-sci
收藏

高压对Y$_{0.7}$Er$_{0.3}$Fe$_2$D$_{4.2}$化合物中显著巡游电子行为的影响

Influence of high pressure on the remarkable itinerant electron behaviour in Y$_{0.7}$Er$_{0.3}$Fe$_2$D$_{4.2}$ compounds

Z. Arnold, O. Isnard, V. Paul-Boncour

AI总结:

本研究针对Y$_{0.7}$Er$_{0.3}$Fe$_2$D$_{4.2}$化合物的特殊磁特性,通过不同压力与磁场下的磁测量,揭示了Er与Fe亚晶格磁相变的压力依赖性及二者的强解耦行为,深化了对巡游电子变磁行为的认识。

摘要:

单斜晶系Y$_{0.7}$Er$_{0.3}$Fe$_2$D$_{4.2}$化合物表现出不寻常的磁特性,存在多种不同的场致磁相变。该氘化物在低温下呈亚铁磁性,且Er亚晶格与Fe亚晶格在不同温度下发生磁相变。Er磁矩在T$_{Er}$=55 K以下有序排列,而Fe磁矩在高达T$_{M0}$=66 K的温度范围内始终保持铁磁耦合。在T$_{M0}$处,Fe磁矩通过巡游电子变磁(IEM)行为发生急剧的铁磁-反铁磁(FM-AFM)相变,该行为对任何体积变化都极为敏感。当温度高于T$_N$=125 K时,Y$_{0.7}$Er$_{0.3}$Fe$_2$D$_{4.2}$变为顺磁性。\n\n通过在最高0.49 GPa的静水压下进行磁测量,我们提取了T$_{Er}$和T$_{M0}$随压力的变化关系。在B=0.03 T的磁场下,两个温度均随施加的压力线性下降,其中dT$_{Er}$/dP=-126 K·GPa$^{-1}$,dT$_{M0}$/dP=-140 K·GPa$^{-1}$。Er磁有序与Fe铁磁有序均在P=0.44(4) GPa时消失。然而,在更大的外加磁场B=5 T下,dT$_{M0}$/dP=-156 K·GPa$^{-1}$,而dT$_{Er}$/dP=-134 K·GPa$^{-1}$,表明二者对压力和磁场的敏感性更弱。在2 K时,饱和磁化强度随压力下降可归因于倾斜和/或晶体场效应导致的平均Er磁矩减小。在T$_{M0}$以上,磁化曲线表现出从反铁磁态到铁磁态的变磁行为,该行为同样对外加压力非常敏感。随加热过程线性升高的转变场B$_{trans}$,在施加压力时向更低温度偏移,0到0.11 GPa之间的偏移量为dT=-17 K。这些结果表明,Er和Fe磁亚晶格随温度、外加磁场和压力的变化表现出强烈的解耦特性。

英文摘要:

Monoclinic Y$_{0.7}$Er$_{0.3}$Fe$_2$D$_{4.2}$ compound exhibits unusual magnetic properties with different field induced magnetic transitions. The deuteride is ferrimagnetic at low temperature and the Er and Fe sublattices present magnetic transitions at different temperatures. The Er moments are ordered below T$_{Er}$=55 K, whereas the Fe moments remain ferromagnetically coupled up to T$_{M0}$ = 66 K. At T$_{M0}$ the Fe moments display a sharp ferromagnetic-antiferromagnetic transition (FM-AFM) through an itinerant electron metamagnetic (IEM) behaviour very sensitive to any volume change. Y$_{0.7}$Er$_{0.3}$Fe$_2$D$_{4.2}$ becomes paramagnetic above T$_N$=125 K. The pressure dependence of T$_{Er}$ and T$_{M0}$ have been extracted from magnetic measurements under hydrostatic pressure up to 0.49 GPa. Both temperatures decrease linearly upon applied pressure with dT$_{Er}$/dP=-126 and dTM0/dP=-140 K.GPa$^{-1}$ for a field of B=0.03 T. Both magnetic Er and ferromagnetic Fe order disappear at P=0.44(4) GPa. However, under a larger applied field B=5 T, dT$_{M0}$/dP=-156 K.GPa$^{-1}$ whereas dT$_{Er}$/dP=-134 K.GPa$^{-1}$ showing a weaker sensitivity to pressure and magnetic field. At 2 K the decrease of the saturation magnetization under pressure can be attributed to a reduction of the mean Er moment due to canting and/or crystal field effect. Above T$_{M0}$ the magnetization curves display a metamagnetic behaviour from AFM to FM state, which is also very sensitive to the applied pressure. The transition field B$_{trans}$, which increases linearly upon heating, is shifted to lower temperature upon applied pressure with dT=-17 K between 0 and 0.11 GPa. These results show a strong decoupling of the Er and Fe magnetic sublattices versus temperature, applied field and pressure.