采用溶胶-凝胶技术合成了原始封端与未封端硫化锌的纳米晶样品。通过 X 射线衍射技术确认了样品的纳米晶性;随着封端剂十二烷基硫酸钠摩尔浓度(x = 0.00、0.02、0.03、0.04 Mol)的增加,颗粒尺寸减小。所得晶粒尺寸分别处于 4.6 nm 至 2.7 nm 的范围内。利用紫外-可见光谱技术估算样品的光学带隙,带隙值处于 3.8 eV 至 4.4 eV 范围内。与块体样品相比,所有样品均表现出量子限域行为。荧光(FL)光谱在约 434 nm、520 nm、545 nm、628 nm 和 694 nm 的发射波长处显示出三个发射峰。FL 强度与封端剂浓度成正比。
英文摘要:
Nanocrystalline samples of pristine capped and uncapped zinc sulphide were synthesized via the sol-gel technique. The nanocrystallinity of the samples were confirmed by the X-ray diffraction technique, where size of the particle size decreases with the increasing of mol. concentration (x = 0.00, 0.02, 0.03, 0.04 Mol). of capping agent sodium dodecyle sulphate. The obtained crystallite sizes were found to be in the range 4.6 nm to 2.7 nm respectively. The optical band gaps of the samples were estimated by using ultra-violet visible spectroscopic techniques and the band gap values were in the range 3.8 eV to 4.4 eV. All the samples showed quantum confinement behavior compared to bulk sample. Fluorescence (FL) spectra showed three emission peaks at the emission wavelengths around 434 nm, 520 nm, 545 nm, 628 nm, and 694 nm. The FL intensities were proportional to the concentration of capping agent.
PEG- and PVP-assisted wet-chemical synthesis of ZnS nanocrystals via hydrothermal and co-precipitation methods for route-dependent structural and bandgap tuning
Ghulam Ishaq Khan Institute of Engineering Sciences and Technology(古拉姆·伊沙克汗工程科学与技术学院);University of Illinois Urbana-Champaign(伊利诺伊大学厄巴纳-香槟分校)
Chemical synthesis and magnetic properties of monodisperse cobalt ferrite nanoparticles
在这项工作中,一个成功的合成磁性钴铁氧体(CoFe 2 O 4)纳米粒子。合成的CoFe 2 O 4纳米粒子具有球形形状,在所选择的溶剂中高度单分散。研究了不同反应条件如温度、反应时间和不同封端剂对产物物相和形貌的影响。扫描透射电子显微镜显示,这些纳米粒子的大小可以通过改变反应条件来控制。X射线衍射和能量色散X射线光谱证实了立方对称的CoFe 2 O 4尖晶石结构的形成。由于优化的反应参数,每个纳米颗粒被证明是一个单一的磁畴的直径范围从6到16 nm。最后,磁性研究表明,所获得的纳米粒子是超顺磁性的小矫顽力值约315 Oe和饱和磁化强度为58 emu/g在室温下。这些结果使得钴铁氧体纳米颗粒有望用于先进的磁性纳米器件和生物磁性应用。
Rapid synthesis of uniformly small nickel nanoparticles for the surface functionalization of epitaxial graphene
NEST, Istituto Nanoscienze–CNR and Scuola Normale Superiore(NEST,意大利国家研究委员会纳米科学研究所和比萨高等师范学院);Department of Physical Science, Earth, and Environment, University of Siena(锡耶纳大学地球与环境物理科学学院);Graphene Laboratories, Istituto Italiano di Tecnologia(意大利理工大学石墨烯实验室)
提出一种以 CTAB 为封端剂、在水溶液中快速合成平均约 11 nm 均匀 Ni 纳米颗粒的方法,并验证其可用于外延石墨烯表面功能化且在 550°C 下保持结构稳定。
Iowa State University(爱荷华州立大学);Ames National Laboratory(艾姆斯国家实验室);National Synchrotron Light Source II, Brookhaven National Laboratory(布鲁克海文国家实验室,国家同步光源二号)