AI总结:

本文提出用加速中性原子束技术在300毫米晶圆尺度上对铌表面氧化物进行可控工程化,以替代天然氧化物,减少微波损耗,有望提升超导量子电路的相干时间。

摘要:

可扩展量子计算的一个主要障碍是量子比特与缺陷相关的双能级系统(TLS)相互作用引起的相位退相干和能量弛豫。量子器件中使用的超导金属表面存在的天然氧化物被公认是降低量子比特相干时间的TLS来源。通过表面工程减少微波损耗(即用具有可预测特性的薄而稳定的表面替代超导金属不受控制的天然氧化物)可以成为推动更高品质因数器件性能向前发展的关键使能因素。在这项工作中,我们提出了一种新方法,利用室温工艺在300毫米晶圆尺度上采用加速中性原子束(ANAB)技术,将铌的天然氧化物(通常在其原始表面暴露于空气时以不受控制的方式形成)替换为工程氧化物。该ANAB束由氩和氧的混合物组成,每个原子的能量可调,并在晶圆表面进行光栅扫描。研究发现,ANAB工程化的Nb氧化物厚度根据ANAB工艺参数在2纳米至6纳米之间变化。变能XPS数据建模证实了ANAB工艺对Nb表面氧化物的厚度和成分控制。这些结果与透射电子显微镜和X射线反射法的结果具有良好相关性。由于ANAB广泛适用于材料表面,本研究表明其有望用于超导量子电路表面的改性,以实现更长的相干时间。

英文摘要:

A major roadblock to scalable quantum computing is phase decoherence and energy relaxation caused by qubits interacting with defect-related two-level systems (TLS). Native oxides present on the surfaces of superconducting metals used in quantum devices are acknowledged to be a source of TLS that decrease qubit coherence times. Reducing microwave loss by surface engineering (i.e., replacing uncontrolled native oxide of superconducting metals with a thin, stable surface with predictable characteristics) can be a key enabler for pushing performance forward with devices of higher quality factor. In this work, we present a novel approach to replace the native oxide of niobium (typically formed in an uncontrolled fashion when its pristine surface is exposed to air) with an engineered oxide, using a room-temperature process that leverages Accelerated Neutral Atom Beam (ANAB) technology at 300 mm wafer scale. This ANAB beam is composed of a mixture of argon and oxygen, with tunable energy per atom, which is rastered across the wafer surface. The ANAB-engineered Nb-oxide thickness was found to vary from 2 nm to 6 nm depending on ANAB process parameters. Modeling of variable-energy XPS data confirm thickness and compositional control of the Nb surface oxide by the ANAB process. These results correlate well with those from transmission electron microscopy and X-ray reflectometry. Since ANAB is broadly applicable to material surfaces, the present study indicates its promise for modification of the surfaces of superconducting quantum circuits to achieve longer coherence times.