arXiv 2301.10306cond-mat.supr-con
收藏

成核与非成核外延α-钽薄膜中的双能级系统

Two-Level Systems in Nucleated and Non-Nucleated Epitaxial alpha-Tantalum films

L. D. Alegria, D. M. Tennant, K. R. Chaves, J. R. I. Lee, S. R. O'Kelley, Y. J. Rosen, J L DuBois

AI总结:

本研究对比了高温生长与室温Nb成核的外延α-钽薄膜谐振器,发现Nb成核薄膜因缺陷密度较高导致双能级系统损耗更大,表明提升Ta薄膜晶体有序性可延长量子比特相干时间。

摘要:

构建具有实用相干性的超导量子处理器取决于减少其构成材料中的损耗。钽(Tantalum)和铌(niobium)一样,已被证明可用作高相干量子比特中的主要超导层。但是,与Nb不同的是,在薄膜沉积过程中,通常需要使用高温来稳定理想的体心立方相,即α-Ta(alpha-Ta)。人们早就知道,一层薄的Nb层可以实现α-Ta的室温成核,尽管在本研究之前,尚未有关于Nb成核Ta薄膜的外延工艺或少光子微波损耗测量的报道。我们比较了由高温(500 °C)生长的Ta薄膜和室温成核的薄膜制成的谐振器,以了解晶体有序性对量子相干性的影响。在这两种情况下,薄膜均以Al2O3 (001) || Ta (110)方式生长,表明外延取向与温度无关,并且在Nb/Ta界面上得以保持。我们使用常规的低功率光谱学测量双能级系统(TLS)损耗,并使用电场偏置技术测量谐振器表面中TLS的有效偶极矩。在我们的测量中,Nb成核的Ta谐振器具有更大的损耗角正切(1.5 +/- 0.1 x 10^-5),高于非成核的Ta谐振器(5 +/- 1 x 10^-6),其比例大致与X射线衍射(0.27 ° vs 0.18 ° [110]反射宽度)和电子显微镜(30 nm vs 70 nm畴尺寸)表征的缺陷密度相对应。损耗角正切对畴尺寸的依赖性表明,开发更有序的Ta薄膜可能会提高量子比特的相干时间。此外,低温α-Ta外延可能能够实现新型无微态异质结构的生长,而这些结构通常无法承受高温加工过程。

英文摘要:

Building usefully coherent superconducting quantum processors depends on reducing losses in their constituent materials. Tantalum, like niobium, has proven utility as the primary superconducting layer within highly coherent qubits. But, unlike Nb, high temperatures are typically used to stabilize the desirable body-centered-cubic phase, alpha-Ta, during thin film deposition. It has long been known that a thin Nb layer permits the room-temperature nucleation of alpha-Ta, although neither an epitaxial process nor few-photon microwave loss measurements have been reported for Nb-nucleated Ta films prior to this study. We compare resonators patterned from Ta films grown at high temperature (500 °C) and films nucleated at room temperature, in order to understand the impact of crystalline order on quantum coherence. In both cases, films grew with Al2O3 (001) || Ta (110) indicating that the epitaxial orientation is independent of temperature and is preserved across the Nb/Ta interface. We use conventional low-power spectroscopy to measure two level system (TLS) loss, as well as an electric-field bias technique to measure the effective dipole moments of TLS in the surfaces of resonators. In our measurements, Nb-nucleated Ta resonators had greater loss tangent (1.5 +/- 0.1 x 10^-5) than non-nucleated (5 +/- 1 x 10^-6) in approximate proportion to defect densities as characterized by X-ray diffraction (0.27 ° vs 0.18 ° [110] reflection width) and electron microscopy (30 nm vs 70 nm domain size). The dependence of the loss tangent on domain size indicates that the development of more ordered Ta films is likely to lead to improvements in qubit coherence times. Moreover, low-temperature alpha-Ta epitaxy may enable the growth of new, microstate-free heterostructures which would not withstand high temperature processing.