常压下Al-Cu-Co合金液相线温度和过冷度的集中行为
Concentration behavior of liquidus temperatures and undercooling of Al-Cu-Co at normal pressure
摘要:
对成分范围为15 at.%的Al-Cu-Co合金进行了差热分析Co和10至30原子% Cu和25 at.% Co和2.5至20原子%本文研究了常压下缓慢冷却(冷却速率为1 K s ~(-1))坩埚晶化过程中固相形成的特点。在Al-Cu-Co系15 at.% Co和25原子% Cu的浓度部分已经建成,这使得可以确定的浓度范围,从不同的阶段形成的结晶的第一阶段。沿不同相区的边界,在液相线上观察到极值。所观察到的极值上的液相线和浓度依赖性的过冷度与变化的化学短程顺序在所考虑的浓度在液体和固体状态。
英文摘要:
Differential thermal analysis has been conducted for the Al-Cu-Co alloys with the composition range of 15 at.% Co and 10 to 30 at.% Cu, and 25 at.% Co and 2.5 to 20 at.% Co. The features of the formation of solid phases have been studied during the crystallization in a crucible in the conditions of slow cooling (rate of cooling to 1 K s-1) at normal pressure. On the state diagram of the Al-Cu-Co system with 15 at.% Co and 25 at.% Cu the concentration sections have been built, which allows to determine the concentration ranges from which different phases are formed during the first stage of crystallization. Along the boundaries of different phase regions, extrema are observed on the liquidus line. The observed extrema on the liquidus lines and concentration dependences of undercooling are associated with change in the chemical short-range order at the considered concentrations both in the liquid and solid states.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。