91钢焊接接头蠕变内应力分析--同步辐射DRX试验与模型

Internal stresses analysis on welded joint in Grade 91 steel under creep test: synchrotron DRX tests and modelling

Solenne Collomb Xiaolei Chen, Jean-Philippe Tinnes, Thomas Schenk, Olivier Ferry, Tsareva Svetlana, Abdelkrim Redjaïmia, Alain Jacques

摘要:

对91钢焊接接头蠕变损伤的分析和认识是能源行业的一个重要课题。在600 $^{\circ}$ C、100 MPa下对焊接接头进行蠕变试验,然后在预期寿命的0%、10%、30%、50%、80%和失效后中断。蠕变损伤的特征在于仅位于临界热影响区(ICHAZ)中样品核心的空洞带。在蠕变条件下,使用\textit{in situ}同步加速器XRD沿焊接接头测试这些样品的不同蠕变寿命。试验结果表明,焊接接头具有明显的应变演化和蠕变损伤特征,且在热影响区(HAZ)有一个局部极大值。在此之后,进行有限元蠕变应变分析与实验结果进行比较。

英文摘要:

The analysis and understanding of creep damage of Grade 91 steel welded joints is an important topic in the energy industry. Creep tests on welded joints were carried out at 600$^{\circ}$C, 100MPa and then interrupted at 0%, 10%, 30%, 50%, 80% of the expected life and after failure. Creep damage is characterised by cavity bands located exclusively in the core of the sample in the InterCritical Heat Affected Zone (ICHAZ). These samples were tested using \textit{in situ} synchrotron XRD along the welded joint under creep conditions for the different creep life time. The experimental results show a significant strain evolution and creep damage characteristic on the welded joint, with a local maximum at the Heat Affected Zone (HAZ). Following this, a finite element creep strain analysis was performed for comparison with the experimental results.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑