Mn(II)阳离子在碱性介质中氧化生成纯水钠锰矿的条件
Conditions for the formation of pure birnessite during the oxidation of Mn(II) cations in aqueous alkaline medium
摘要:
以MnO 4-、Mn 2+和OH-为原料,通过氧化还原反应合成水钠锰矿。Mn(VII):选择Mn(II)比为0.33,并使用三种方法,包括在剧烈搅拌下快速混合三种试剂中的两种,然后逐滴加入第三种。用XRD、FTIR和XPS对所得固体进行了表征。它们的平均氧化态测定从ICP和CEC测量,而它们的表面性质进行了研究,通过XPS。这项研究提供了更多的理解溶解氧在水钠锰矿和黑锰矿的形成的重要性,并显示了获得纯水钠锰矿的方法。反离子的作用。还检查了Na+或K+。
英文摘要:
Birnessite was synthetized through redox reaction by mixing MnO4-, Mn2+ and OH- solutions. The Mn(VII): Mn(II) ratio of 0.33 was chosen and three methods were used consisting in a quick mixing under vigorous stirring of two of the three reagents and then on the dropwise addition of the third one. The obtained solids were characterized by XRD, FTIR and XPS spectroscopies. Their average oxidation states were determined from ICP and CEC measurements while their surface properties were investigated by XPS. This study provides an increased understanding of the importance of dissolved oxygen in the formation of birnessite and hausmannite and shows the ways to obtain pure birnessite. The role of counter-ion ie. Na+ or K+ was also examined.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。