用于能量收集应用的铅镁石酸-钛酸铅(PMN-0 .3PT)压电陶瓷的结构和机电特性
Structural and electromechanical characterization of lead magnesium niobate-lead titanate (PMN-0.3PT) piezoceramic for energy harvesting applications
摘要:
利用压电效应原理的高效机械能收集需要特定的材料性能要求。这包括大压电电荷系数(dij)、大弹性应变(εy)、小弹性柔量(Sij)和小介电常数(\k{appa} ij)的组合。本工作进行结构,电气,机械,和机电特性的无焦宝石铅镁石-钛酸铅(1-x)[Pb(Mg(1/3)Nb(2/3)O3)]-xPbTiO 3在x = 0.3或PMN-0.3 PT,估计上述关键参数的机械能收获。采用固相反应法合成了无焦磷酸盐的PMN-0.3PT陶瓷,其单斜相(Pm和Cm)共存。压电电荷系数(d33)、介电常数(\k{appa} 33 ^T)、弹性顺应性(s33 ^E)和机电耦合系数(k33)分别估计为200 pC/N(约)、1.06(约)x 10^-8 F/m、13.16(约)x 10^-12 m2/N和0.54(约),在规定尺寸的极化样品上使用室温阻抗测量(EN 50324-1:2002和CEI/IEC 60483:1976)。极化泄漏,由于运输的各种带电缺陷被确定为负责降低机电性能相比,单晶体的报告。PMN-0.3PT的弹性应变(εy)与柔性(fFOM)估计为4.5 x 10-4。动态机械负载下的能量收集显示最大短路电流密度为95 nA/cm 2,开路电场为98 V/cm。PMN-0.3PT陶瓷以其优异的性能成为压电能量收集的重要材料。
英文摘要:
Efficient mechanical energy harvesting using the principle of piezoelectric effect demands specific material-property requirements. This includes a combination of large piezoelectric charge coefficient (dij), large elastic strain (εy), small elastic compliance (Sij), and small dielectric permittivity (\k{appa}ij). The present work undertakes structural, electrical, mechanical, and electromechanical characterization of pyrochlore-free lead magnesium niobate-lead titanate (1-x)[Pb(Mg(1/3)Nb(2/3)O3)]-xPbTiO3 at x = 0.3 or PMN-0.3PT, to estimate the above critical parameters for mechanical energy harvesting. Pyrochlore-free PMN-0.3PT ceramic with co-existing monoclinic (Pm and Cm) phases was synthesized using solid-state reaction method. Piezoelectric charge coefficient (d33), dielectric permittivity (\k{appa}33^T), elastic compliance (s33^E), and electromechanical coupling factor (k33), were estimated to be, 200 pC/N (approx), 1.06 (approx) x 10^-8 F/m, 13.16 (approx) x 10^-12 m2/N, and 0.54 (approx), respectively, using room temperature impedance measurement on a poled sample with specified dimensions (EN 50324-1:2002 and CEI/IEC 60483:1976). Polarization leakage due to transport of various charged defects was identified to be responsible for the reduced electromechanical properties compared to those reported for single crystals. Elastic strain (εy) vis-à-vis flexibility (fFOM) of the PMN-0.3PT was estimated to be 4.5 x 10-4. Energy harvesting under dynamic mechanical loading shows a maximum short-circuit current density, 95 nA/cm2, and an open-circuit electric field, 98 V/cm. With its impressive performance, PMN-0.3PT ceramic constitutes an important material for piezoelectric energy harvesting.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。