高载流子密度条件下过氧化物降解机理研究

Degradation Mechanism of Perovskite under High Charge Carrier Density Condition

Guohui Li, Huihui Pi, Yanfu Wei, Bolin Zhou, Ya Gao, Rong Wen, Yuying Hao, Han Zhang, Beng S. Ong, Yanxia Cui

摘要:

广泛的研究集中在低载流子密度(<10^16 cm^-3)下钙钛矿的降解,但很少调查高载流子密度(~10^18 cm^-3)下的降解机理。在这里,我们研究了高载流子条件下钙钛矿的降解机制。与以前的工作中的观察,我们发现,MAPbI 3的退化开始在表面缺陷和进展从表面缺陷向邻近区域的高载流子密度条件下。通过使用PbI 2钝化,缺陷引发的降解被显著抑制,并且纳米片以逐层方式降解,使得MAPbI 3激光器能够持续4500 s(2.7*10^7脉冲),这几乎是未钝化的纳米片激光器的3倍长。同时,具有纳米片腔的PbI 2钝化MAPbI 3纳米片激光器显示出高达~7800的最大品质因数,这是所有MAPbI 3纳米片腔报道的最高品质因子。此外,基于双重钝化策略,通过同时延缓缺陷引发的降解和表面引发的降解,证明了可以持续8500 s(5.1*10^7脉冲)的高稳定性MAPbI 3纳米片激光器。这项工作为理解高载流子密度下钙钛矿的降解提供了深入的见解。

英文摘要:

Extensive studies have focused on degradation of perovskite at low charge carrier density (<10^16 cm^-3), but few have surveyed the degradation mechanism at high charge carrier density (~10^18 cm^-3). Here, we investigate the degradation mechanisms of perovskite under high charge carrier conditions. Unlike the observations in previous works, we find that MAPbI3 degradation starts at surface defects and progressing from the surface defects towards neighboring regions under high charge carrier density condition. By using PbI2 passivation, the defect-initiated degradation is significantly suppressed and the nanoplatelet degrades in a layer-by-layer way, enabling the MAPbI3 laser sustain for 4500 s (2.7*10^7 pulses), which is almost 3 times longer than that of the nanoplatelet laser without passivation. Meanwhile, the PbI2 passivated MAPbI3 nanoplatelet laser with the nanoplatelet cavity displaying a maximum quality factor up to ~7800, the highest reported for all MAPbI3 nanoplatelet cavities. Furthermore, a high stability MAPbI3 nanoplatelet laser that can last for 8500 s (5.1*10^7 pulses) is demonstrated based on a dual passivation strategy, by retarding the defect-initiated degradation and surface-initiated degradation, simultaneously. This work provides in-depth insights for understanding the degradation of perovskite at high charge carrier density.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑