Ni-(Fe,Co)-Mn-(Al,In)快淬薄带的显微组织及相关力学性能研究

Microstructure and correlated mechanical properties study of Ni-(Fe, Co)-Mn-(Al, In) as-spun ribbons

Chunyang Zhang, Laureline Porcar, Salvatore Miraglia, Patricia Donnadieu, Muriel Braccini, Richard Haettel, Marc Verdier

摘要:

Ni-Mn基记忆合金作为一种很有前途的弹性热材料,已有大量的文献报道,尤其是大量的体样品研究。初生薄带具有更大的表面积和更有效的传热,很少被研究,因此具有重要意义。在本工作中,我们成功地生产了很长的Ni-Fe-Mn-(Al,In)快淬带,长度约为300毫米。通过扫描电子显微镜/电子背散射衍射(SEM/EBSD)、纳米压痕和三点弯曲实验,研究了这些薄带的微观结构和力学性能。通过SEM/EBSD分析,研究了快淬薄带的显微组织和织构。由于快速凝固过程中的温度梯度,沿薄带厚度方向(TD)存在组织梯度,导致在快淬过程中沿与旋转轮接触的表面形成细小的等轴晶,而在快淬过程中,沿旋转轮接触的表面形成细长晶粒。等轴晶和细长晶均具有较强的{001}纤维织构(<001>//TD)。纳米压痕分析表明,两种不同的显微组织之间的硬度变化不大。Ni-Fe-Mn-Al和Ni-Fe-Mn-In薄带的塑性指数均在金属间化合物范围内。用Al取代In可以使延展性指数略有增加,可达到0.75。在三点弯曲试验中,细小等轴晶的抗拉性能优于细长晶。用Al替代In使最大弯曲应变提高了3倍。Ni-Fe-Mn-Al快淬薄带断裂前的最大应变可达3%。断口形貌分析表明,沿晶断裂是这些快淬薄带的主要损伤机制。

英文摘要:

The Ni-Mn-based shape memory alloys as a promising candidate of elastocaloric material has been reported in many literatures, especially on bulk samples. The as-spun ribbon, which has a larger surface area and is more efficient for heat transfer, is rarely studied and hence of importance. In the present work, we succeeded in producing very long as-spun Ni-Fe-Mn-(Al, In) ribbons, with around 300 mm in length. The microstructure and mechanical properties of these as-spun ribbons were thoroughly investigated by scanning electron microscopy / electron backscattered diffraction (SEM/EBSD), nanoindentation and 3-points bending experiments. Through SEM/EBSD analyses, the microstructure and texture of the as-spun ribbons were studied. A gradient in microstructure exists along the thickness direction (TD) of the ribbon, which is induced by the temperature gradient during fast rate solidification, resulting in fine equiaxed grains along the surface contacted with the rotating wheel in melt spinning process and elongated grains, respectively. Both equiaxed and elongated grains possess a strong {001} fiber texture (<001>//TD). Nanoindentation analyses show little variation of hardness between the two different microstructures. The ductility index of both Ni-Fe-Mn-Al and Ni-Fe-Mn-In ribbons are within the range of intermetallic materials. The substitution of In by Al allows to increase very slightly the ductility index, which can reach 0.75. The fine equiaxed grains show better tensile resistance than the elongated grains in 3-points bending test. The substitution of In by Al improves the maximum bending strain by a factor of 3. The maximum strain for Ni-Fe-Mn-Al as-spun ribbons can reach 3 % before fracture. Fractography shows that the intergranular fracture is the main damage mechanism in these as-spun ribbons.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑