聚合物的断裂力学行为:1.非晶玻璃态

Fracture mechanical behavior of polymers: 1. Amorphous glassy state

Travis Smith, Chaitanya Gupta, Caleb Carr, Shi-Qing Wang

摘要:

对玻璃态聚合物的断裂行为进行了理论分析和实验研究。我们的双折射测量量化了在不同阶段的拉伸过程中在切割尖端的局部应力积累。基于聚甲基丙烯酸甲酯(PMMA),双酚A聚碳酸酯(PC)和聚对苯二甲酸乙二醇酯(PET),我们发现了几个关键的结果超出了现有的知识基础。(1)固有断裂强度和屈服强度σ_F(inh)和σ_Y(inh)与断裂应力和屈服应力(σ_b和σ_y)在量值上差别很小。(2)在接近切割尖端时,预切割附近的应力增强(SI)与线弹性断裂力学(LEFM)的理论描述偏离。(3)SI满足一个自然截止值,低于该值应力停止增加。(4)对于所有三种聚合物和不同的切口尺寸a,切口尖端的应力条带都显示出随远场载荷s 0近似线性增加的趋势。(5)从stip和KI之间的线性关系中出现了特征长度尺度P。(6)脆性聚合物的断裂韧性可用临界应力强度因子K_Ic = sigma_F(inh)(2*pi*P)~(1/2)表征,揭示了这两个关键量的相关性。(7)脆性玻璃聚合物如PMMA的临界能量释放率GIc由其断裂功wF(未切割试样的)和P的乘积确定。(8)在文献中定义为G_Ic/w_F的难以捉摸的断裂内聚长度Lfc自然地来自(7)中所述的G_Ic的新表达式,即,这些结果表明,大量的未来的工作是需要获得更多的了解与断裂和塑料的故障行为。

英文摘要:

Theoretical analyses and experiments have been carried out to investigate fracture behavior of glassy polymers. Our birefringence measurements quantify the local stress buildup at cut tip during different stages of drawing. Based on polymethyl methacrylate (PMMA), bisphenol A polycarbonate (PC) and polyethylene terephthalate (PET), we find several key results beyond the existing knowledge base. (1) The inherent fracture and yield strengths sigma_F(inh) and sigma_Y(inh) differ little in magnitude from the breaking and yield stress (sigma_b and sigma_y). (2) Stress intensification (SI) near a pre-through-cut builds up deviates from the theoretical description of linear elastic fracture mechanics (LEFM) upon approaching the cut tip. (3) SI meets a natural cutoff below which stress ceases to increase. (4) The stress stip at cut tip shows a trend of approximate linear increase with the far-field load s0 for all three polymers and different cut size a. (5) A characteristic length scale P emerges from the linear relation between stip and KI. For these glassy polymers, P is on the order of 0.1 mm. (6) Fracture toughness of brittle polymers is characterized by critical stress intensity factor K_Ic = sigma_F(inh)(2*pi*P)1/2, revealing relevance of the two crucial quantities. (7) The critical energy release rate GIc for brittle glass polymers such as PMMA is determined by the product of its work of fracture wF (of uncut specimen) and P. (8) The elusive fractocohesive length Lfc defined in the literature as G_Ic/w_F naturally arises from the new expression for G_Ic as stated in (7), i.e., it is essentially P. These results suggest that a great deal of future work is required to acquire additional understanding with regards to fracture and failure behaviors of plastics.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑