注入铒的硅中的自旋回波
Spin echo from erbium implanted silicon
AI总结:
本研究针对注入铒的硅量子技术平台,测量其5K下的自旋弛豫与相干时间,揭示自旋回波调制源于Er³+与29Si核的超超精细相互作用,明确T2受谱扩散限制及对应铒中心的结构。
摘要:
注入铒的硅作为量子技术平台,兼具电信与集成电路工艺兼容性。在铒浓度为3×10^17 cm^-3、氧浓度为10^20 cm^-3的注入硅中,5 K温度下测得电子自旋相干时间T2为7.5 μs,自旋-晶格弛豫时间T1约为1 ms。自旋回波衰减曲线呈现强调制,这与Er³+和29Si核自旋库之间的超超精细相互作用一致。计算得到的谱扩散时间与测得的T2相近,表明T2受限于由邻近Er³+自旋的T1诱导翻转导致的谱扩散。该回波的起源是被六个氧原子包围、具有单斜C1h格位对称性的铒中心。
英文摘要:
Erbium implanted silicon as a quantum technology platform has both telecommunications and integrated circuit processing compatibility. In Si implanted with Er to a concentration of 3x10^17 cm^3 and O to a concentration of 10^20 cm^3, the electron spin coherence time, T2, and the spin-lattice relaxation time, T1, were measured to be 7.5 ls and ~1 ms, respectively, at 5 K. The spin echo decay profile displayed strong modulation, which was consistent with the super-hyperfine interaction between Er3þ and a spin bath of 29Si nuclei. The calculated spectral diffusion time was similar to the measured T2, which indicated that T2 was limited by spectral diffusion due to T1-induced flips of neighboring Er3þ spins. The origin of the echo is an Er center surrounded by six O atoms with monoclinic C1h site symmetry.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。