中熵NiCo(CrAl)合金提高室温和高温力学性能的微结构工程

Microstructural engineering of medium entropy NiCo(CrAl) alloy for enhanced room and high-temperature mechanical properties

Nithin Baler, Abdulla Samin M, Akshat Godha, Surendra Kumar Makineni

摘要:

这项工作演示了一个强大的和韧性的中熵合金的发展,采用传统的合金化和热机械加工诱导部分再结晶(PR)和析出强化的显微组织。电子显微镜和原子探针层析成像的结合使用揭示了在此过程中的微观结构演变的顺序。首先,均匀化合金的冷加工导致高度变形的显微组织。在700°C下退火时,B2有序沉淀物在高度取向错误的位点上非均匀地成核。这些B2促进新的再结晶的无应变晶粒的粒子刺激成核(PSN)。再结晶晶界的迁移导致高密度层状组织中L12有序区的不连续析出。原子尺度的成分分析表明,显着量的Ni局限于GB区域之间的B2和L12沉淀,表明镍作为一个速率控制元素粗化的微观结构。在20小时的退火时,该合金包括软再结晶区和硬非再结晶区的复合微观结构、晶界(GB)处的B2颗粒和晶粒内的共格L12沉淀物。B2在再结晶期间固定GB运动,而后者提供高强度。该显微组织在环境温度下的0.2%屈服应力(YS)值为1030 MPa,伸长率为32%,并且在670°C下保持高达910 MPa。此外,它在700 °C下显示出出色的微观结构稳定性,并在高达770°C的高温下抗变形。变形显微组织的检查揭示了过度的孪晶、堆垛层错的形成、L12沉淀物的剪切以及归因于合金的高应变硬化的在B2沉淀物和GB周围的位错的积累。

英文摘要:

This work demonstrates the development of a strong and ductile medium entropy alloy by employing conventional alloying and thermomechanical processing to induce partial recrystallization (PR) and precipitation strengthening in the microstructure. The combined usage of electron microscopy and atom probe tomography reveals the sequence of microstructural evolution during the process. First, the cold working of homogenized alloy resulted in a highly deformed microstructure. On annealing at 700°C, B2 ordered precipitates heterogeneously nucleate on the highly misoriented sites. These B2 promotes particle stimulated nucleation (PSN) of new recrystallized strain-free grains. The migration of recrystallized grain boundaries leads to discontinuous precipitation of L12 ordered regions in highly dense lamellae structures. Atomic-scale compositional analysis reveals a significant amount of Ni confined to the GB regions between B2 and L12 precipitates, indicating Ni as a rate-controlling element for coarsening the microstructure. On 20 hours of annealing, the alloy comprises a composite microstructure of soft recrystallized and hard non-recrystallized zones, B2 particles at the grain boundaries (GBs), and coherent L12 precipitates inside the grains. The B2 pins the GB movement during recrystallization while the latter provides high strength. The microstructure results in a 0.2% yield stress (YS) value of 1030 MPa with 32% elongation at ambient temperature and retains up to 910 MPa at 670°C. Also, it shows exceptional microstructural stability at 700 °C and resistance to deformation at high temperatures up to 770°C. Examination of deformed microstructure reveals excessive twinning, formation of stacking faults, shearing of L12 precipitates, and accumulation of dislocations at around the B2 precipitates and GBs attributed to high strain hardening of the alloy.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑