Y33 66.67- xAlx(0 <= x <= 33.33)体系相态及吸氢性能的研究
Investigation of the phase occurrence and H sorption properties in the Y33.33Ni66.67-xAlx (0 <= x <= 33.33) system
摘要:
在0 <= x <= 33.3范围内研究了Y33.33Ni66.67-xAlx系统。合金采用感应熔炼法合成。用X射线粉末衍射仪(XRD)研究了其物相组成和结构特性。用XRD和电子探针分析(EPMA)研究了Al在各相中的溶解度。在473 K下通过压力-组成等温线和动力学曲线表征了催化剂的加氢性能。当x = 0时,Y33.33Ni66.67合金为立方超结构,空间群为F4- 3 m,Y空位有序。当x = 1.67 ≤ x ≤ 8.33时,合金主要由Y(Ni,Al)2和Y(Ni,Al)3伪二元相组成,而当x = 16.67 ≤ x ≤ 33.33时,合金主要由三元线化合物Y3 Ni 6Al 2,Y2 Ni 2Al和YNiAl组成。与二元化合物Y33.33Ni66.67相反,Y(Ni,Al)2伪二元化合物以C15相(Fd-3 m空间群)存在,Y空位无序。Al在C15 YNi 2-yAly相中的溶解度极限为y = 0.11(即,x = 3.67)。当x从5.00增加到6.67时,Y(Ni,Al)3相从菱方(PuNi 3型,R-3 m)转变为六方(CeNi 3型,P63/mmc)结构。氢化后,C_(15)Y(Ni,Al)_2的不平衡以及YNi和Y_2Ni_2Al结晶度的损失是导致Y_(33.33)Ni_(66.67-x)Al_x(0 ≤ x ≤ 33.33)合金循环容量衰减的主要原因。
英文摘要:
The Y33.33Ni66.67-xAlx system has been investigated in the region 0 <= x <= 33.3. The alloys were synthesized by induction melting. Phase occurrence and structural properties were studied by X-Ray powder Diffraction (XRD). The Al solubility in each phase has been investigated by XRD and Electron Probe Micro-Analysis (EPMA). The hydrogenation properties were characterized by pressure-composition isotherm measurements and kinetic curves at 473 K. For x = 0, the binary Y33.33Ni66.67 alloy crystallizes in the cubic superstructure with F4-3m space group and ordered Y vacancies. For 1.67 <= x <= 8.33, the alloys contain mainly Y(Ni, Al)2 and Y(Ni, Al)3 pseudobinary phases; while for 16.67 <= x <= 33.33 they are mainly formed by ternary line compounds Y3Ni6Al2, Y2Ni2Al and YNiAl. Contrary to the binary Y33.33Ni66.67, Y(Ni, Al)2 pseudo-binary compounds crystalize in C15 phase (space group Fd-3m ) with disordered Y vacancies. The solubility limit of Al in the C15 YNi2-yAly phase is y = 0.11 (i.e., x = 3.67). The Y(Ni, Al)3 phase changes from rhombohedral (PuNi3-type, R-3m) to hexagonal (CeNi3-type, P63/mmc) structure for x increasing from 5.00 to 6.67. Upon hydrogenation, the disproportion of C15 Y(Ni, Al)2 and losses of crystallinity of YNi and Y2Ni2Al are the main reasons causing capacity decay of Y33.33Ni66.67-xAlx (0 <= x <= 33.33) alloys upon cycling.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。