骨科用可吸收聚乳酸/镁纤维复合材料的强度、耐腐蚀性和细胞反应
Strength, corrosion resistance and cellular response of interfaces in bioresorbable poly-lactic acid/Mg fiber composites for orthopedic applications
摘要:
研究了聚乳酸/镁纤维复合材料在模拟体液中浸泡后纤维/基体界面的剪切强度和耐腐蚀性能。界面的剪切强度通过在垂直于纤维的复合材料薄片中的推出测试来测量。结果表明,复合材料在模拟体液中浸泡148 h后,界面强度从15.2 \pm 1.4 MPa下降到7.8 \pm 3.7 MPa。当水通过聚合物扩散到界面时,界面强度的降低与纤维的快速腐蚀有关。由于腐蚀产物的形成而导致的纤维膨胀足以促进聚合物基质中的径向裂纹,这促进了水的进入和纤维中腐蚀点的发展。此外,对材料的细胞培养测试表明,由于纤维腐蚀产生的局部环境变化,镁纤维的早期降解影响了镁纤维附近的前成骨细胞的增殖。因此,镁纤维的表面改性,以延迟降解似乎是一个关键点,为进一步发展镁/聚乳酸复合材料的生物医学应用。
英文摘要:
The shear strength and the corrosion resistance of the fiber/matrix interface after immersion in simulated body fluid was studied in poly-lactic acid/Mg fiber composites. The shear strength of the interface was measured by means of push-out tests in thin slices of the composite perpendicular to the fibers. It was found that the interface strength dropped from 15.2 \pm 1.4 MPa to 7.8 \pm 3.7 MPa after the composite was immersed in simulated body fluid for 148 hours. The reduction of the interface strength was associated to the fast corrosion of the fibers as water diffused to the interface through the polymer. The expansion of the fibers due to the formation of corrosion products was enough to promote radial cracks in the polymer matrix which facilitate the ingress of water and the development of corrosion pitting in the fibers. Moreover, cell culture testing on the material showed that early degradation of the Mg fibers affected the proliferation of pre-osteoblasts near the Mg fibers due to the local changes in the environment produced by the fiber corrosion. Thus, surface modification of Mg fibers to delay degradation seems to be a critical point for further development of Mg/PLA composites for biomedical applications.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。