壳聚糖对硫酸盐和钙离子富集溶液中镍的选择性强化吸附
Selective and enhanced nickel adsorption from sulfate- and calcium-rich solutions using chitosan
摘要:
镍(Ni)是一种经济上重要的金属,其特征在于其机械强度和抗腐蚀性能。随着工业对镍的需求不断增加和可获得的镍原生矿石的枯竭,需要可持续的技术来从替代资源中回收这种金属。在这项研究中,使用壳聚糖吸附作为一个可持续的技术,以回收硫酸盐(SO 42-)和钙(Ca)丰富的二次资源镍。在批实验中的pH值,接触时间,和SO 42-和Ca的存在下对Ni吸附的影响进行了研究。进行化学形态建模,以分析在不同条件下存在的主要Ni物种如何影响吸附过程的效率。壳聚糖的最大镍吸附容量的比较,在不存在(1.00 mmol/g)和存在(1.49 mmol/g)的500 mM的SO 42-和10 mM的钙表明这些离子对镍吸附的积极影响。X射线光电子能谱学(XPS)分析表明,Ni/SO_4 ~(2-)体系中(NiSO_4)_0物种的存在促进了壳聚糖对Ni的吸附。然而,动力学研究证实,Ni吸附速率下降了4.5倍时,SO 42-的存在。随后的连续吸附从一个真正的SO 42-丰富的浸出液中的柱设置显示,壳聚糖是选择性的Ni超过Ca和Cr的选择性比为9.6(KNi/Ca)和3.0(KNi/Cr)。总体而言,本研究表明Ni与SO 42-的络合增强了壳聚糖对Ni的吸附能力,但减慢了吸附过程。
英文摘要:
Nickel (Ni) is an economically important metal characterized by its mechanical strength and anticorrosion properties. With the increasing industrial demand for Ni and the depleting accessible Ni primary ores, sustainable technologies are required for the recovery of this metal from alternative resources. In this study, adsorption using chitosan was investigated as a sustainable technique to recover Ni from sulfate (SO42-) and calcium (Ca) rich secondary resources. The effects of pH, contact time, and the presence of SO42- and Ca on Ni adsorption were investigated in batch experiments. Chemical speciation modeling was performed to analyze how the predominant Ni species present under different conditions may affect the efficiency of the adsorption process. The comparison of the maximum Ni adsorption capacities of chitosan in the absence (1.00 mmol/g) and presence (1.49 mmol/g) of 500 mM SO42- and 10 mM Ca indicated the positive effect of these ions on Ni adsorption. The predominance of the neutrally charged (NiSO4)0 species in Ni/SO42- system has contributed to the enhanced Ni adsorption on chitosan as verified by X-ray photoelectron spectroscopy (XPS) analysis. However, kinetic studies confirmed that the Ni adsorption rate decreased by 4.5 times when SO42- was present. The subsequent continuous Ni adsorption from a real SO42-rich leachate in a column setup revealed that chitosan is selective for Ni over Ca and Cr with selectivity quotients of 9.6 (K Ni/Ca) and 3.0 (K Ni/Cr). Overall, this study indicated that Ni complexation with SO42- enhances the Ni adsorption capacity of chitosan, but slows down the adsorption process.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。