arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2106.15926physics.app-phcond-mat.mtrl-sci
收藏

降低冶金级硅中的陷阱和沉淀:磷扩散吸杂的影响

Reduction of Trapping and Recombination in Upgraded Metallurgical Grade Silicon: Impact of Phosphorous Diffusion Gettering

N. Dasilva-Villanueva, S. Catalán-Gómez, D. Fuertes Marrón, J. J. Torres, M. García-Corpas, C. del Cañizo

摘要:

升级冶金级(UMG)硅(Si)由于其低成本、低环境影响和低资本支出而引起了人们作为太阳能电池的替代材料的兴趣。已经报道了在从高纯度多晶硅获得的水平上的最大电池效率。然而,较高的缺陷密度和补偿掺杂特性导致基于UMG的电池效率在频率分布图中在更宽的范围内变化。在这份报告中,我们的特点mc-Si UMG样品具有不同的缺陷密度,将它们与单晶硅UMG和商业高性能mc-Si样品进行比较,分析载流子捕获的光电导(PC)衰减测量的影响,以及它的演变后,应用磷扩散吸杂(PDG)过程。当分析PC测量的衰减时间常数时,在mc-Si样品中发现慢(66.8 ± 14.3ms)和快(16.1 ± 3.5ms)陷阱,而在单UMG样品中没有发现陷阱的证据。在PDG过程之后,慢陷阱被有效地去除,而快陷阱仍然存在。位错团簇的影响和氧的可能作用,所揭示的傅立叶变换红外光谱(FTIR)进行了讨论。最后,由于PDG处理的少数载流子寿命的改善,报告了每种样品类型,在没有慢陷阱的mc-Si样品中达到高达140 us的值,

英文摘要:

Upgraded metallurgical grade (UMG) silicon (Si) has raised interest as an alternative material for solar cells due to its low cost, low environmental impact and low CAPEX. Maximum cell efficiencies at the level of those obtained from high purity poly-Si have been reported. However, a higher defect density and the compensated doping character result in UMG-based cell efficiencies varying over wider ranges in frequency distribution charts. In this report we characterize mc-Si UMG samples with different defect densities, comparing them with mono-Si UMG and commercial high-performance mc-Si samples, analysing the impact of carrier trapping by means of photoconductance (PC) decay measurements, and its evolution after applying a phosphorous diffusion gettering (PDG) process. When analyzing the decay time constant of the PC measurements, slow (66.8+-14.3 ms) and fast (16.1+-3.5 ms) traps are found in mc-Si samples, while no evidence of trapping is found in mono-UMG samples. Slow traps are effectively removed after the PDG process, while fast traps do remain. The influence of dislocations clusters and the possible role of oxygen, as revealed by Fourier-transform infrared spectroscopy (FTIR) is discussed. Finally, the improvement in minority carrier lifetime due to the PDG treatment is reported for each sample type, reaching values up to 140 us in mc-Si samples with no slow traps neither interstitial oxygen FTIR-peaks

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑