摘要:

已知V $_3$ Si薄膜是超导的,其转变温度高达15 K,这取决于退火温度和下面的衬底的性质。在这里,我们调查的薄膜结构特性的前景进一步集成在硅技术的量子线路。已经确定了两个挑战:(i)V $_3$ Si和Si衬底之间的热膨胀率的大差异导致热处理后的大的热应变,以及(ii)当V $_3$ Si沉积在硅上时形成不期望的硅化物相VSi $_2$。第一种是通过在蓝宝石和氧化硅晶片上沉积200 nm V $_3$ Si层来研究的,这两种晶片都不与硅化物反应。然后将这些样品在室温至860°C之间加热和冷却,在此期间进行原位XRD测量。分析揭示了一个高度非线性的应力发展过程中的结晶和随后的晶粒生长,以及硅化物和衬底之间的热膨胀失配的贡献加热,而在冷却过程中的薄膜表现出热弹性。第二个挑战是通过在体硅上沉积20、50、100和200 nm的V $_3$ Si膜来探索的。对于每个厚度,制备六个样品,然后在500 ° C和750°C之间的温度下退火,随后测量其电阻率、剩余电阻比和超导临界温度。对于至少100 nm的硅化物厚度,确定了工艺窗口,在该工艺窗口内,需要在V $_3$ Si膜的质量和由VSi $_2$的形成引起的其消耗之间进行权衡。

英文摘要:

V$_3$Si thin films are known to be superconducting with transition temperatures up to 15 K, depending on the annealing temperature and the properties of the substrate underneath. Here we investigate the film structural properties with the prospect of further integration in silicon technology for quantum circuits. Two challenges have been identified: (i) the large difference in thermal expansion rate between V$_3$Si and the Si substrate leads to large thermal strains after thermal processing, and (ii) the undesired silicide phase VSi$_2$ forms when V$_3$Si is deposited on silicon. The first of these is studied by depositing layers of 200 nm V$_3$Si on wafers of sapphire and oxidized silicon, neither of which react with the silicide. These samples are then heated and cooled between room temperature and 860°C, during which in-situ XRD measurements are performed. Analysis reveals a highly non-linear stress development during heating with contributions from crystallization and subsequent grain growth, as well as the thermal expansion mismatch between silicide and substrate, while the film behaves thermoelastically during cooling. The second challenge is explored by depositing films of 20, 50, 100 and 200 nm of V$_3$Si on bulk silicon. For each thickness, six samples are prepared, which are then annealed at temperatures between 500 and 750°C, followed by measurements of their resistivity, residual resistance ratio and superconducting critical temperature. A process window is identified for silicide thicknesses of at least 100 nm, within which a trade-off needs to be made between the quality of the V$_3$Si film and its consumption by the formation of VSi$_2$.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑