高热通量疲劳下碳纤维复合材料瓦与金属散热器连接的损伤证据
Evidence of damage in carbon fibre composite tiles joined to a metallic heat sink under high heat flux fatigue
摘要:
两年的Active Metal Casting平板焊接经验表明,该技术适用于Tore Supra(10 MW/m ${}^2$)中预期的热通量。测试进行了多达3330次循环,元件仍然起作用。在较高的热通量下,观察到疲劳损伤,但粘合剂抵抗得非常好,没有瓷砖脱落。对这种故意损坏的连接进行检查,发现有分布的裂缝,证明没有任何薄弱环节。对这些较高热通量的限制更多地与设计和基底材料有关,而不是与粘合剂本身有关。
英文摘要:
The two years experience with Active Metal Casting flat bonds shows that this technology is suitable for the heat fluxes expected in Tore Supra (10 MW/m${}^2$). Tests were pursued up to 3330 cycles, with elements still functional. At higher heat fluxes, fatigue damage is observed, but the bond resists remarkably well with no tile detachment. Examination of such deliberately damaged bonds showed distributed cracking, proving the absence of any weak link. The limitations to those higher heat fluxes are more related to the design and the base materials than to the bond itself.