arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2010.00293cond-mat.mtrl-scicond-mat.mes-hall
收藏

Ti 1 s X射线吸收光谱研究Ti3AlC2 MAX相和Ti3C2Tx MXene中的局域化学键和结构性质

Local chemical bonding and structural properties in Ti3AlC2 MAX phase and Ti3C2Tx MXene probed by Ti 1s X-ray absorption spectroscopy

Martin Magnuson, Lars-Åke Näslund

摘要:

利用X射线吸收近边结构(XANES)和扩展X射线吸收精细结构(EXAFS)研究了过渡金属碳化物MAX相Ti 3AlC 2和MXene Ti 3C 2 Tx中的化学键。MAX相是固有的纳米层压材料,其由Mn+1Xn的交替层和周期表中IIIA或IVA族的A元素的单层组成,其中M是过渡金属,X是碳或氮。用表面终止物质Tx代替A元素将分离Mn+1Xn层,形成Mn+1XnTx的二维(2D)薄片。对于Ti 3C 2 Tx,Tx对应于覆盖每个单个2D Mn+1Xn薄片的两侧的氟(F)和氧(O)。Ti_3AlC_2和Ti_3C_2Tx的K边(1 s)XANES均表现出C_(2 p)- Ti_(3d)杂化的特征边前吸收区,具有清晰的晶场分裂,而主边吸收特征源于Ti_(1 s)-> 4p激发,其中只有后者对终止物种的fcc位占据表现出敏感性。从EXAFS得到的配位数表明,Ti 3AlC 2和Ti 3C 2 Tx是高度各向异性的强平面内的贡献Ti和动态的平面外的贡献从铝单层和终止物种,分别。如温度依赖性测量所示,随着温度从室温升高到750 °C,O的贡献向较短的键长移动,而F减小。

英文摘要:

The chemical bonding within the transition-metal carbide materials MAX phase Ti3AlC2 and MXene Ti3C2Tx is investigated by X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS) spectroscopies. MAX phases are inherently nanolaminated materials that consist of alternating layers of Mn+1Xn and monolayers of an A-element from the IIIA or IVA group in the periodic table, where M is a transition metal and X is either carbon or nitrogen. Replacing the A-element with surface termination species Tx will separate the Mn+1Xn-layers forming two-dimensional (2D) flakes of Mn+1XnTx. For Ti3C2Tx the Tx corresponds to fluorine (F) and oxygen (O) covering both sides of every single 2D Mn+1Xn-flake. The Ti K-edge (1s) XANES of both Ti3AlC2 and Ti3C2Tx exhibit characteristic pre-edge absorption regions of C 2p - Ti 3d hybridization with clear crystal-field splitting's while the main-edge absorption features originate from the Ti 1s -> 4p excitation, where only the latter shows sensitivity towards the fcc-site occupation of the termination species. The coordination numbers obtained from EXAFS show that Ti3AlC2 and Ti3C2Tx are highly anisotropic with a strong in-plane contribution for Ti and with a dynamic out-of-plane contribution from the Al monolayers and termination species, respectively. As shown in the temperature-dependent measurements, the O contribution shifts to shorter bond length while the F diminishes as the temperature is raised from room temperature up to 750 °C.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑