在VECC制备同位素富集的$^{112,116,120,124}$ Sn靶
Preparation of Isotopically enriched $^{112,116,120,124}$Sn targets at VECC
摘要:
采用电阻加热和机械轧制方法分别制备了同位素富集的116 Sn(~380 μg/cm ~ 2)、124 Sn(~400 μg/cm ~ 2)薄靶箔和112 Sn(1.7mg/cm ~ 2)、120 Sn(1.6mg/cm ~ 2)厚靶箔。在薄靶的制备过程中,材料量少的富集靶的制备、薄靶释放剂的选择以及沉积材料在溶剂中的分离是几个挑战之一。用~(241)Am α源测量了靶的均匀性。在薄靶的制备中,NaCl被用作释放剂。这些靶已成功地用于VECC的核物理实验。
英文摘要:
Resistive heating and mechanical rolling methods have been employed to prepare isotopically enriched thin target foils of 116Sn (~380 μg/cm2), 124Sn(~400 μg/cm2) and thicker foils of 112Sn (1.7 mg/cm2),120Sn (1.6 mg/cm2),respectively. Preparation of enriched targets with small amount of material, selection of releasing agent for thin targets and separation of deposited material insolvent were among the several challenges while fabrication of the thin targets. Uniformity of the targets has been measured using 241Am α-source. NaCl has been used as releasing agent in preparation of the thin targets. These targets have been successfully used in nuclear physics experiments at VECC.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。