$\text{Bi}/\text{TiO}_{2}$核壳纳米线的半金属-半导体转变

Semimetal to semiconductor transition in $\text{Bi}/\text{TiO}_{2}$ core/shell nanowires

M. Kockert, R. Mitdank, H. Moon, J. Kim, A. Mogilatenko, S. H. Moosavi, M. Kroener, P. Woias, W. Lee, S. F. Fischer

摘要:

我们展示了完整的热电和结构表征的个别铋基(Bi基)核/壳纳米线。研究了应变对不同直径的铋/二氧化钛($\text{Bi}/\text{TiO}_{2}$)纳米线的电导率、绝对塞贝克系数和热导率的温度依赖性的影响,并与铋(Bi)、铋/碲(Bi/Te)纳米线和铋块体进行了比较。在表面、晶体缺陷和核与壳之间的界面处的散射将室温下的电导率降低到小于$5\,\%$,并将热导率降低到小于体积值的$25\,\%$至$50\,\%$。代表压缩应变,$\text{Bi}/\text{TiO}_{2}$核/壳纳米线显示出与Bi和Bi/Te纳米线相反的随着温度降低而降低的电导率。我们发现,由$\text{TiO}_{2}$壳引起的压缩应变可以导致铋的能带打开,在室温下,与体相相比,绝对塞贝克系数由$10\,\%$增加到$30\,\%$。在半导体状态下,活化能被确定为$\left|41.3\pm0.2\right|\,\text{meV}$。我们表明,如果应变超过弹性极限的半金属状态恢复由于晶格弛豫。

英文摘要:

We demonstrate the full thermoelectric and structural characterization of individual bismuth-based (Bi-based) core/shell nanowires. The influence of strain on the temperature dependence of the electrical conductivity, the absolute Seebeck coefficient and the thermal conductivity of bismuth/titanium dioxide ($\text{Bi}/\text{TiO}_{2}$) nanowires with different diameters is investigated and compared to bismuth (Bi) and bismuth/tellurium (Bi/Te) nanowires and bismuth bulk. Scattering at surfaces, crystal defects and interfaces between the core and the shell reduces the electrical conductivity to less than $5\,\%$ and the thermal conductivity to less than $25\,\%$ to $50\,\%$ of the bulk value at room temperature. On behalf of a compressive strain, $\text{Bi}/\text{TiO}_{2}$ core/shell nanowires show a decreasing electrical conductivity with decreasing temperature opposed to that of Bi and Bi/Te nanowires. We find that the compressive strain induced by the $\text{TiO}_{2}$ shell can lead to a band opening of bismuth increasing the absolute Seebeck coefficient by $10\,\%$ to $30\,\%$ compared to bulk at room temperature. In the semiconducting state, the activation energy is determined to $\left|41.3\pm0.2\right|\,\text{meV}$. We show that if the strain exceeds the elastic limit the semimetallic state is recovered due to the lattice relaxation.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑