等离子体增强原子层沉积低电阻率镍纳米管及三维自旋电子学相干磁化动力学
Plasma-enhanced atomic layer deposition of nickel nanotubes with low resistivity and coherent magnetization dynamics for 3D spintronics
摘要:
我们报道了等离子体增强原子层沉积(ALD)制备保形镍薄膜和纳米管,使用二茂镍作为前体,水作为氧化剂和循环等离子体增强还原步骤与氢。优化的ALD脉冲序列,结合后处理退火处理,使我们能够制备30 nm厚的金属Ni层,在室温下的电阻率为8 $μΩ$ cm,在平面衬底和纳米模板上具有良好的共形性。因此,我们制备了几个微米长的镍纳米管的直径范围从120到330 nm。我们报告ALD生长和功能特性的个别镍纳米管的磁输运和自旋波模式的限制方面的相关性。研究结果提供了新的观点,镍基自旋电子学和磁振子设备在GHz频率制度与3D设备架构。
英文摘要:
We report plasma-enhanced atomic layer deposition (ALD) to prepare conformal nickel thin films and nanotubes by using nickelocene as a precursor, water as the oxidant agent and an in-cycle plasma enhanced reduction step with hydrogen. The optimized ALD pulse sequence, combined with a post-processing annealing treatment, allowed us to prepare 30 nm thick metallic Ni layers with a resistivity of 8 $μΩ$cm at room temperature and good conformality both on the planar substrates and nanotemplates. Thereby we fabricated several micrometer-long nickel nanotubes with diameters ranging from 120 to 330 nm. We report on the correlation between ALD growth and functional properties of individual Ni nanotubes characterized in terms of magneto-transport and the confinement of spin wave modes. The findings offer novel perspectives for Ni-based spintronics and magnonic devices operated in the GHz frequency regime with a 3D device architecture.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。