嵌在纤锌矿GaAs纳米线壳层中的圆柱形限制MnAs纳米晶的铁磁性增强
Enhanced ferromagnetism in cylindrically confined MnAs nanocrystals embedded in wurtzite GaAs nanowire shells
摘要:
在嵌入纤锌矿GaAs基质中的应变MnAs纳米晶体中,铁磁相变温度提高了近30%。纤锌矿GaAs施加拉伸应力的六方晶系的MnAs纳米晶体,防止六方晶系的正交结构的相变,这在体MnAs与磁性相结合。这种效应导致磁结构相变温度从块状MnAs的313 K显著地移动到张力应变MnAs纳米晶体的400 K以上。这一发现得到了最先进的透射电子显微镜、灵敏磁力计和第一性原理计算的证实。该效应依赖于定义分子束外延生长的核-多壳纤锌矿(Ga,In)As/(Ga,Al)As/(Ga,Mn)As/GaAs纳米线的纳米管几何形状,其中MnAs纳米晶体在热处理诱导的纤锌矿(Ga,Mn)As相分离成GaAs:MnAs颗粒系统期间形成。两种类型的六方晶格的这种独特的组合提供了在MnAs中获得准流体静力拉伸应变的可能性(否则不可能),导致该化合物中的实质性铁磁相变温度增加。
英文摘要:
Nearly 30% increase of the ferromagnetic phase transition temperature has been achieved in strained MnAs nanocrystals embedded in a wurtzite GaAs matrix. Wurtzite GaAs exerts tensile stress on hexagonal MnAs nanocrystals, preventing a hexagonal to orthorhombic structural phase transition, which in the bulk MnAs is combined with the magnetic one. This effect results in a remarkable shift of the magneto-structural phase transition temperature from 313 K in the bulk MnAs to above 400 K in the tensely strained MnAs nanocrystals. This finding is corroborated by the state of the art transmission electron microscopy, sensitive magnetometry and the first-principles calculations. The effect relies in defining a nanotube geometry of molecular beam epitaxy grown core-multishell wurtzite (Ga,In)As/(Ga,Al)As/(Ga,Mn)As/GaAs nanowires where the MnAs nanocrystals are formed during the thermal-treatment-induced phase separation of wurtzite (Ga,Mn)As into the GaAs:MnAs granular system. Such a unique combination of two types of hexagonal lattices provides possibility of attaining quasi-hydrostatic tensile strain in MnAs (impossible otherwise), leading to the substantial ferromagnetic phase transition temperature increase in this compound.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。