用低能电子图案化Sn基EUV抗蚀剂
Patterning Sn-based EUV resists with low-energy electrons
摘要:
极紫外(EUV)光刻是将用于半导体工业中的亚20纳米规模的印刷电路的最新技术。在用EUV光子(92 eV)照射抗蚀剂材料时产生的低能电子(LEE)在纳米粒子的形成中起核心作用。然而,到目前为止,这一过程的细节还没有得到很好的理解。在这项工作中,一种新的实验方法,结合低能电子显微镜(LEEM),电子能量损失谱(EELS),和原子力显微镜(AFM)被用来研究在0-40 eV范围内的分子有机金属EUV抗蚀剂的薄膜中的电子引起的变化被称为锡氧笼。LEEM-EELS光谱实验用于检测电子暴露后的表面充电,并估计电子着陆能量。AFM曝光后的分析表明,抗蚀剂与LEE的照射导致抗蚀剂层的致密化与碳损失。在平版印刷应用中,产生致密化的相同化学过程使得溶解度变化导致斑图形成。值得注意的是,低至1.2eV的电子能够在Sn基抗蚀剂中诱导化学反应。基于LEE曝光在3-48 mC/cm 2剂量范围内产生的厚度分布,提出了一个简化的反应模型,其中抗蚀剂经历连续的化学反应,首先产生稀疏的交联网络,然后形成更密集的交联网络。该模型使我们能够估计的最大反应体积的初始材料的0.15纳米3每个入射电子的能量范围内的研究,这意味着,平均每个分子需要不到10 LEE变成不溶性的材料,从而呈现图案。
英文摘要:
Extreme Ultraviolet (EUV) lithography is the newest technology that will be used in the semiconductor industry for printing circuitry in the sub-20 nm scale. Low-energy electrons (LEEs) produced upon illumination of resist materials with EUV photons (92 eV) play a central role in the formation of the nanopatterns. However, up to now the details of this process are not well understood. In this work, a novel experimental approach that combines Low-Energy Electron Microscopy (LEEM), Electron Energy Loss Spectroscopy (EELS), and Atomic Force Microscopy (AFM) is used to study changes induced by electrons in the 0-40 eV range in thin films of molecular organometallic EUV resists known as tin-oxo cages. LEEM-EELS spectroscopic experiments were used to detect surface charging upon electron exposure and to estimate the electron landing energy. AFM post-exposure analyses revealed that irradiation of the resist with LEEs leads to the densification of the resist layer associated to carbon loss. The same chemical processes that yield densification render the solubility change responsible for the pattern formation in the lithographic application. Remarkably, electrons as low as 1.2 eV are able to induce chemical reactions in the Sn-based resist. Based on the thickness profiles resulting from LEE exposures in the 3-48 mC/cm 2 dose range, a simplified reaction model is proposed where the resist undergoes sequential chemical reactions, yielding first a sparsely cross-linked network, followed by the formation of a denser cross-linked network. This model allows us to estimate a maximum reaction volume on the initial material of 0.15 nm 3 per incident electron in the energy range studied, which means that less than 10 LEEs per molecule on average are needed to turn the material insoluble and thus render a pattern.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。