arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1909.12779physics.app-phphysics.ins-det
收藏

等离子体轮廓飞行时间质谱用于半导体结构的快速元素分析,具有纳米范围的深度分辨率

Plasma Profiling Time-of-Flight Mass Spectrometry for Fast Elemental Analysis of Semiconductor Structures with Depth Resolution in the Nanometer Range

Hendrik Spende, Christoph Margenfeld, Tobias Meyer, Irene Manglano Clavero, Heiko Bremers, Andreas Hangleiter, Michael Seibt, Andreas Waag, Andrey Bakin

摘要:

等离子体飞行时间质谱(PP-TOFMS)最近获得了兴趣,因为它能够在短的采集时间内以高的深度分辨率对半导体结构进行元素分析。正如Tempez等人最近所示,PP-TOFMS可用于获得现代场效应晶体管结构中的成分[1]。在那里,将结果与传统的SIMS测量进行了比较。在本研究中,我们比较PP-TOFMS测量的Al-/In-/GAN量子阱多叠层建立的微米和纳米分析技术,如阴极发光(CL),扫描透射电子显微镜(STEM),能量色散X射线光谱(EDX)和X射线衍射(XRD)。我们表明,PP-TOFMS是能够解决的层结构的样品,甚至超过500 nm深的样品,并允许测定的相对元素组成的准确度约为10 rel。%.因此,它是一种非常快速的替代方法,以获得半导体元素的深度分布,而不需要昂贵和耗时的样品制备,因为它是TEM所需要的。此外,PP-TOFMS提供比例如电化学电容-电压(ECV)更好的深度分辨率和更多的元素信息,因为所有元素的采集并行发生,并且不仅观察到电(ECV)或光学(CL)活性元素。

英文摘要:

Plasma profiling time of flight mass spectrometry (PP-TOFMS) has recently gained interest, as it enables the elemental profiling of semiconductor structures with high depth resolution in short acquisition times. As recently shown by Tempez et al., PP-TOFMS can be used to obtain the composition in the structures for modern field effect transistors [1]. There, the results were compared to conventional SIMS measurements. In the present study, we compare PP-TOFMS measurements of an Al-/In-/GaN quantum well multi stack to established micro- and nano-analysis techniques like cathodoluminescence (CL), scanning transmission electron microscopy (STEM), energy dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD). We show that PP-TOFMS is able to resolve the layer structure of the sample even more than 500 nm deep into the sample and allows the determination of a relative elemental composition with an accuracy of about 10 rel. %. Therefore, it is an extremely rapid alternative method to obtain semiconductor elemental depth profiles without expensive and time consuming sample preparation as it is needed for TEM. Besides, PP-TOFMS offers better depth resolution and more elemental information than for example electrochemical capacitance-voltage (ECV), as the acquisition of all elements occurs in parallel and not only electrically (ECV) or optically (CL) active elements are observed.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑