环境稳定的缺陷钝化过氧化物酶室温连续波激光
Environmentally Stable Room Temperature Continuous Wave Lasing in Defect-passivated Perovskite
摘要:
金属卤化物钙钛矿已经成为光子集成电路(PIC)中片上激光器的有前途的增益材料。然而,在室温下光泵浦下稳定的连续波(CW)激光行为-电泵浦激光的先决条件-尚未得到证明。为了实现稳定的CW操作,我们引入了多种策略,包括CH 3 NH3 PbBr 3(MAPbBr 3)薄膜的形态,结构和界面工程,以提高钙钛矿的本征稳定性,以及高质量的腔设计,以降低操作功率。我们首次证明,超过90分钟长的绿色连续激光与9.4 W/cm 2阈值从聚碳酸酯(PC)的缺陷钝化,直接图案化MAPbBr 3二维光子晶体(PhC)腔没有任何衬底冷却。我们还展示了我们的方法对MAPbBr 3电激励下的性能的有效性:我们观察到通过将我们的策略应用于MAPbBr 3 LED,电流效率提高了七倍。这项工作为在钙钛矿中实现电泵浦激光铺平了道路。
英文摘要:
Metal halide perovskites have emerged as promising gain materials for on-chip lasers in photonic integrated circuits (PICs). However, stable continuous wave (CW) lasing behavior under optical pumping at room temperature - a prerequisite for electrically pumped lasing - has not yet been demonstrated. To achieve stable CW operation, we introduce a multiplex of strategies that include morphological, structural and interfacial engineering of CH3NH3PbBr3 (MAPbBr3) thin films to improve perovskite's intrinsic stability, as well as high quality cavity design to reduce the operational power. We demonstrate for the first time, over 90-minute-long green CW lasing with 9.4W/cm2 threshold from a polycarbonate (PC)-defect-passivated, directly patterned MAPbBr3 two-dimensional photonic crystal (PhC) cavity without any substrate cooling. We also show our approach's effectiveness on the performance of MAPbBr3 under electrical excitation: we observe a seven-fold current efficiency enhancement by applying our strategies to a MAPbBr3 LED. This work paves the way to the realization of electrically pumped lasing in perovskites.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。