PMMA海泡石纳米双孔材料的力学性能
Mechanical properties of PMMA sepiolite nanocellular materials with a bimodal cellular structure
摘要:
通过固态发泡生产具有微米和纳米尺寸(300至500 nm)泡孔的双峰泡孔聚(甲基丙烯酸甲酯),其具有至多5重量%的海泡石纳米颗粒和50重量%至75重量%的孔隙率。进行单轴压缩试验以测量海泡石浓度对固体和蜂窝状纳米复合材料的弹性模量和屈服强度的影响。进行单边缺口弯曲试验,以将固体和蜂窝状纳米复合材料的断裂韧性与海泡石浓度相关联。当考虑完整的孔隙度范围时,相对模量与海泡石含量无关。相比之下,通过添加海泡石颗粒观察到相对模量的温和增强,用于具有接近50%的孔隙率的发泡纳米复合材料。蜂窝状纳米复合材料的相对压缩强度作为海泡石浓度的函数温和地降低。观察到通过添加海泡石的相对断裂韧性的强烈增强。相对断裂韧性和相对模量(在50%孔隙率下)的增强可归因于由于发泡和在发泡期间微米尺寸的聚集体从固相向微孔孔的迁移而改善的颗粒分散。
英文摘要:
Bimodal cellular poly(methyl methacrylate) with micron and nano sized (300 to 500 nm) cells with up to 5 weight percent of sepiolite nanoparticles and porosity from 50 weight percent to 75 weight percent are produced by solid state foaming. Uniaxial compression tests are performed to measure the effect of sepiolite concentration on the elastic modulus and the yield strength of the solid and cellular nanocomposites. Single edge notch bend tests are conducted to relate the fracture toughness of the solid and cellular nanocomposites to sepiolite concentration. The relative modulus is independent of sepiolite content to within material scatter when considering the complete porosity range. In contrast, a mild enhancement of the relative modulus is observed by the addition of sepiolite particles for the foamed nanocomposites with a porosity close to 50 percent. The relative compressive strength of the cellular nanocomposites mildly decreases as a function of sepiolite concentration. A strong enhancement of the relative fracture toughness by the addition of sepiolites is observed. The enhancement of the relative fracture toughness and the relative modulus (at 50 percent porosity) can be attributed to an improved dispersion of the particles due to foaming and the migration of micron sized aggregates from the solid phase to the microcellular pores during foaming.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。