晶粒尺寸工程提高无铅BCZT铁电陶瓷介电性能

Enhancement of dielectric properties of lead-free BCZT ferroelectric ceramics by grain size engineering

Zouhair Hanani, Daoud Mezzane, M'barek Amjoud, Sébastien Fourcade, A G Razumnaya, Igor A Luk'yanchuk, Mohamed Gouné

摘要:

无铅Ba0.85Ca0.15Ti0.9Zr0.1O3(BCZT)陶瓷以其优异的介电、铁电和压电性能在微电子器件制造中受到广泛关注。为了了解晶粒尺寸和晶粒尺寸分布对无铅Ba0.85Ca0.15Ti0.9Zr0.1O3(BCZT)弛豫铁电体介电性能的影响,提出了一种新颖的方法.它是基于表面活性剂辅助溶剂热处理结合1250 °C的低温常规烧结。以此方式设计了三种具有不同平均晶粒尺寸和不同晶粒尺寸分布的高致密BCZT。通过控制晶粒尺寸和致密化工艺,获得了介电性能的显著提高。测得的介电常数范围为5370至9646,介电损耗提高了70%。令人惊讶的是,有证据表明,有明确的平均晶粒尺寸与介电性能之间的联系。事实上,已经发现,由于致密化的增强,高密度的细化晶粒的存在导致介电性能的改善。这一工作为铁电材料的设计提供了一种新的思路。

英文摘要:

Lead-free Ba0.85Ca0.15Ti0.9Zr0.1O3 (BCZT) ceramics had attracted much attention for the fabrication of microelectronic devices by virtue of their excellent dielectric, ferroelectric and piezoelectric properties. To understand the effects of both mean grain size and grain size distribution on the dielectric properties of lead-free Ba0.85Ca0.15Ti0.9Zr0.1O3 (BCZT) ferroelectric relaxors, an original method was proposed. It is based on the surfactant-assisted solvothermal processing coupled with low-temperature conventional sintering at 1250 °C. In this way, three highly dense BCZT with different mean grain size and dissimilar grain size distribution were designed. A significant increase of dielectric properties was obtained by a control of grain size and densification process. The dielectric constants measured were ranged from 5370 to 9646 and the dielectric loss was enhanced by 70%. Surprisingly, it was evidenced that there is unequivocal link between mean grain size with dielectric properties. Indeed, it was found that the presence of high density of refined grains leads to an improvement of dielectric properties due to an enhancement of densification. This work may provide a new strategy to design ferroelectric materials with enhanced properties.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑