高压下Fe $_{2}$ TiO $_{4}$后尖晶石中的特定自旋交叉

Site-specific spin crossover in Fe$_{2}$TiO$_{4}$ post-spinel under high pressures to near a megabar

W. M. Xu, G. R. Hearne, S. Layek, D. Levy, J-P. Itié, M. P. Pasternak, G. Kh. Rozenberg, E. Greenberg

摘要:

室温下~90 GPa的X射线衍射研究表明,Fe $_{2}$ TiO $_{4}$亚铁反尖晶石在指定的起始转变压力下经历以下结构转变顺序:立方(Fd 3 m)→四方(I41/amd)→正交(Cmcm)→正交(Pmma)。在Cmcm相内,启动特定于位点的自旋交叉,并且仅涉及构成所有Fe位置的~25%的高度扭曲的八面体位点。这表现为在~40 GPa以上dV/V0 ~ 3.5%的急剧体积减小和在可变低温下在57 Fe穆斯堡尔谱中辨别出的涌现的抗磁性分量。随后的CMCM到Pmma Fe/Ti无序有序重构促进在6倍协调(八面体)网站。其余的高自旋Fe在6倍和8倍的协调网站(约75%的丰度)的Pmma相表现出平均饱和内磁场H $_{hf}$ ~ 42 T到~90 GPa,典型的自旋(轨道淬灭)费米接触值。相比之下,平均H $_{hf}$ ~ 20 T值,表示未淬灭的轨道矩,发生在Cmcm相中低于40-45 GPa的自旋交叉起始区域。因此,网站特定的自旋交叉调用一个合作的晶格响应和多面体的扭曲在其余的高自旋Fe网站,翻译为3d水平(子带)的变化和随之而来的轨道矩淬火。在~90 GPa附近,Fe $_{2}$ TiO $_{4}$是部分自旋转换的化学有序Pmma后尖晶石结构,具有~100 meV的持久电荷间隙。尽管结构对称性的变化,部分自旋交叉和晶格压缩性导致约33%的总减少的晶胞体积和相应的3d带宽加宽,强电子相关持续在高致密化。

英文摘要:

X-ray diffraction studies to ~90 GPa at room temperature show that Fe$_{2}$TiO$_{4}$ ferrous inverse spinel undergoes the following sequence of structural transitions : cubic (Fd3m) to tetragonal (I41/amd)to orthorhombic(Cmcm) to orthorhombic(Pmma),at the indicated onset transition pressures. Within the Cmcm phase, site-specific spin crossover is initiated and involves only highly distorted octahedral sites constituting ~25% of all Fe locations. This is manifest as a steeper volume decrease of dV/V0 ~ 3.5% beyond ~40 GPa and an emergent diamagnetic component discerned in 57Fe Mössbauer spectroscopy at variable cryogenic temperatures. A subsequent Cmcm to Pmma Fe/Ti disorder-order reconfiguration is facilitated at 6-fold coordinated (octahedral) sites. The rest of the high-spin Fe in 6-fold and 8-fold coordinated sites (~75% abundance) in the Pmma phase exhibit average saturation internal magnetic fields of H$_{hf}$ ~ 42 T to ~90 GPa, typical of spin-only (orbitally quenched) Fermi-contact values. By contrast average H$_{hf}$ ~ 20 T values, signifying unquenched orbital moments, occur below the 40-45 GPa spin-crossover initiation regime in the Cmcm phase. Therefore site-specific spin crossover invokes a cooperative lattice response and polyhedral distortions at the rest of the high-spin Fe sites, translating to 3d level (sub-band) changes and consequential orbital moment quenching. Near ~90 GPa Fe$_{2}$TiO$_{4}$ is a partially spin-converted chemically ordered Pmma post-spinel structure having a persistent charge gap of ~100 meV. Despite structural symmetry changes, partial spin crossover and lattice compressibility resulting in a ~33% total reduction in unit-cell volume and corresponding 3d bandwidth broadening, strong electron correlations persist at high densification.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑