arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 1809.07438cond-mat.mtrl-sci
收藏

模型Ni-Al-Mo高温合金相分离过程中的形态、纳米结构和成分演变:原子探针层析实验和晶格动力学蒙特卡罗模拟

Morphological, nanostructural, and compositional evolution during phase separation of a model Ni-Al-Mo superalloy: Atom-probe tomographic experiments and lattice-kinetic Monte Carlo simulations

Yiyou Tu, Zugang Mao, Ronald D. Noebe, David N. Seidman

摘要:

采用原子探针层析成像和晶格动力学蒙特卡罗(LKMC)模拟方法研究了Ni-6.5Al-9.9Mo合金在978 K时效0.125 ~ 1024 h后的相分离过程。纳米结构的时间演变的基础上,确定了三个实验制度:(1)伴随沉淀物成核和生长(t小于0.25小时);(2)并发凝聚和聚结(t0.25至16小时);和(3)准静态粗化的γ '(L12)沉淀物(t16至1024小时)。根据准静态粗化模型的预测,通过实验确定了平均沉淀物半径和沉淀物数密度Nv(t)的时间依赖性,分别为0.344(0.012)和-0.95(0.02)。在978 K时效的合金中,Al强烈地分配到γ '(L12)相,分配系数为4.06(0.04),而Mo和Ni分配到γ(f.c.c.)矩阵的值分别为0.61(0.01)和0.90(0.01)。在准稳态区(t大于16 h),Al、Mo和Ni在γ(f.c.c.)基体和γ ′(L12)沉淀物与多组分粗化模型的预测值-0.33相当一致。边缘到边缘间的沉淀物距离的定量分析表明,凝聚和聚结是周围的γ '(L12)-沉淀物的扩散场的重叠的后果。3-D APT和LKMC结果表明,界面组成宽度随值的增加而减小。无限时效时Ni、Al和Mo的界面组成宽度分别为1.89(0.22)nm、2.09(0.12)nm和2.64(0.03)nm。

英文摘要:

The details of phase separation of a Ni-6.5Al-9.9Mo aged at 978 K for aging times ranging from 0.125 to 1024 h are investigated by atom-probe tomography and lattice-kinetic Monte Carlo (LKMC) simulations. On the basis of the temporal evolution of the nanostructure, three experimental regimes are identified: (1) concomitant precipitate nucleation and growth (t less than 0.25 h); (2) concurrent coagulation and coalescence (t 0.25 to 16 h); and (3) quasi-stationary coarsening of gamma prime(L12)- precipitates (t 16 to 1024 h). The temporal dependencies of the mean precipitate radius and precipitate number density, Nv(t), are determined experimentally, 0.344 (0.012) and -0.95(0.02), respectively, following the predictions of quasi-stationary coarsening models. In this alloy aged at 978 K, Al partitions strongly to the gamma prime(L12)-phase with a partitioning coefficient 4.06(0.04), whereas Mo and Ni partition to the gamma(f.c.c.)-matrix with values of 0.61(0.01) and 0.90(0.01), respectively. In the quasi-stationary regime(t larger than 16h), the temporal exponents of the Al, Mo, and Ni supersaturations in both the gamma(f.c.c.)-matrix and gamma prime(L12)-precipitates are in reasonable agreement with a multi-component coarsening model's prediction of -0.33. Quantitative analyses of the edge-to-edge inter-precipitate distances demonstrate that coagulation and coalescence are consequences of the overlap of the diffusion fields surrounding the gamma prime(L12)-precipitates. Both 3-D APT and LKMC results demonstrate that the interfacial compositional width decrease with increasing values. And the interfacial compositional width at infinite ageing time are estimated to be 1.89(0.22) nm, 2.09(0.12) nm and 2.64(0.03) nm for Ni, Al and Mo, respectively.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑