高性能金属非晶磁性薄片基磁介质电感器
High Performance Metallic Amorphous Magnetic Flake-based Magnetodielectric Inductors
摘要:
通过球磨有效直径为20微米的气体雾化非晶粉末来制备具有高达175比1的纵横比的片状FeSi基金属非晶合金颗粒。起始粉末的饱和磁通量密度Bs为1.5 T,矫顽力Hc为94 A/m。通过研磨工艺参数,例如持续时间、速度以及研磨球的类型、质量和直径来控制薄片的纵横比以及它们的磁性。为了使装料的氧化最小化,将粉末在氩气吹扫的手套箱中处理,在甲苯中研磨,随后在真空中干燥。随后,通过在石蜡或环氧树脂中悬浮和定向FeSi基粉末制备软磁介电复合材料。然后将复合材料压制成环形,用矢量网络分析仪测量其高频复磁导率。考察了片状颗粒长径比和体积含量对复合材料渗透性能的影响。结果表明,复合材料的渗透率随鳞片长径比的增大而增大。例如,对于30体积%的给定加载因子,通过将FeSi基夹杂物的纵横比从1(球体)增加到大于175:1(薄片),复合材料在0.1GHz下的磁导率几乎增加了两倍并接近10的值。
英文摘要:
Flake-shaped FeSi-based metallic amorphous alloy particles, having an aspect ratio as high as 175 to 1, were prepared by ball milling gas atomized amorphous powders of an effective diameter of 20 micrometers. The starting powder had a saturation magnetic flux density, Bs, of 1.5 T and a coercivity, Hc, of 94 A/m. The aspect ratio of the flakes, as well as their magnetic properties, were controlled by milling process parameters, such as duration, speed, and the type, mass and diameter of the milling balls. To minimize the oxidation of the charge, the powders were handled in an argon gas-purged glove box, milled in toluene, and subsequently dried in vacuo. Subsequently, soft magnetodielectric composites were prepared by suspending and aligning the FeSi-based powders in paraffin wax or epoxy resin. The composites were then pressed into toroids for measurements of their high frequency complex permeability by a vector network analyzer. The influence of the flake aspect ratio and volume loading fraction on the permeability of the composites were investigated. Results indicate that the composite permeability increases with the flake aspect ratio. For example, for a given loading factor of 30 vol.%, the composite permeability at 0.1 GHz nearly tripled and approached the value of 10 by increasing the aspect ratio of the FeSi-based inclusions from 1 (spheres) to greater than 175 to 1 (flakes).
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。