热稳定高效储能陶瓷材料(Na0 .5- xKxBi0.5-xLax)TiO3的结构、介电和铁电研究
Structural, dielectric and ferroelectric studies of thermally stable and efficient energy storage ceramic material: (Na0.5-xKxBi0.5-xLax)TiO3
摘要:
研究了溶胶-凝胶自燃烧法合成的无铅(Na 0. 5-xKxBi 0. 5-xLax)TiO 3粉体的结构、介电和铁电性能。同步加速器X射线衍射数据的Rietveld精修证实了对于所有组合物具有R3 c空间群的纯单相菱面体晶体结构,并且反相八面体倾斜角随着组合物X的增加而减小。通过能量色散X射线光谱法确认均匀性和元素比例。随温度变化的介电研究表明,由于晶格中的A位无序,所有样品都存在两种扩散型介电异常,这被归因于两种转变:铁电到反铁电和反铁电到顺电相变。这些相变的转变温度被发现作为组成的函数降低。介电常数的热稳定性范围从~ 100 C增加到220 C作为组成的函数。稳定的介电常数首先从母体化合物的1557 10%增加,随着组成的增加,对于6%的组成,在~180 C至340 C的温度范围内,emid ~ 2508 10%最高,之后对于12%降低到1608 10%,但仍然高于母体化合物Na 0.5Bi 0.5TiO 3。铁电测量表明,由于晶粒尺寸的减小,矫顽场作为组合物的函数单调减小,通过使用场发射扫描电子显微镜的显微结构研究证实。还观察到能量存储效率作为组成的函数从~ 17%到87%的指数增加。这些类型的材料具有稳定的高介电常数和低tan δ,在热稳定介电常数材料和能量存储应用领域具有广阔的范围。
英文摘要:
The structural, dielectric and ferroelectric properties of lead-free (Na0.5-xKxBi0.5-xLax)TiO3 powders synthesized by sol-gel self-combustion method were investigated. Rietveld refinement of Synchrotron x-ray diffraction data confirms pure single phase rhombohedral crystal structure with R3c space group for all the compositions and anti-phase octahedral tilting angle decreased with increase in composition x. Homogeneity and elemental proportions were confirmed by Energy dispersive x-ray spectrometry. The temperature-dependent dielectric study has shown two diffuse type of dielectric anomaly for all the samples, due to A-site disorder in the lattice, which has been assigned to two-has transitions: ferroelectric to anti-ferroelectric and anti-ferroelectric to the paraelectric phase transition. The transition temperature of these phase transitions is found to decrease as a function of composition. Thermal stability range of dielectric constant increases from ~100C to 220C as a function of composition. Stable dielectric constant first increases, from 1557 10 % for parent compound, with the composition, highest for 6 % composition with emid ~ 2508 10 % for the temperature range ~180 C to 340C and after that decreases to 1608 10 % for 12 % but remain higher than the parent compound Na0.5Bi0.5TiO3. Ferroelectric measurements have shown monotonously decreasing coercive field as a function of the composition due to a decrease in grain size, confirmed by microstructural studies using Field Emission Scanning Electron Microscope. Exponential increases in the energy storage efficiency from ~ 17 % to 87 % as a function of composition have also observed. These types of materials, with stable high dielectric constant and low tan delta, have a vast scope in the field of the thermally stable dielectric constant materials and energy storage applications.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。