arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 1805.01343physics.app-phphysics.class-ph
收藏

3D打印PLA和ABS样品的异步锁相热成像

Asynchronous Lock In Thermography of 3D Printed PLA and ABS samples

K. H. H. Goh, Q. F. Lim, P. K. Pallathadka

摘要:

锁相热成像是一种有用的无损检测技术(NDT),用于增强检测组件中的缺陷,因为它放大了缺陷存在的相位对比。与恒定加热相比,发现这种放大约为2-3倍。目前使用的是一台快速沉积建模(FDM)3D打印机来打印具有已知缺陷的样品,以确定不同变量对锁定阶段数据的相对影响。使用ABS(丙烯腈-丁二烯-苯乙烯)和PLA(聚乳酸)打印样品进行比较,并探索诸如打印方向、相机、加热功率、锁定频率以及缺陷的厚度、宽度和深度等变量。发现不同的材料导致不同的基线,但具有相似的相位衬度。一种新的异步技术被开发出来,可以使用5种不同的红外相机进行锁定测量,并得到了类似的结果。即使是便宜的相机,如Seek Thermal CompactXR,也被证明能够检测出与其他相机(如FLIR SC 7500)相同的缺陷。加热功率不影响相位对比度,但深度不超过1.0 mm的较浅缺陷除外,其中较高的功率会产生更好的对比度。正如预期的那样,较深的缺陷只能使用较低的锁定频率来检测,并且对于较宽、较厚和较浅的缺陷存在更好的相位对比。结果表明,基于相位信号趋势,宽度为4 mm的缺陷可以自动检测到约1.5 mm的深度。帧数据的二次采样显示,每个锁定期至少需要10帧,以使锁定相位对比的偏差最小。此外,还表明,只要第一帧与加热循环同步,对于深度高达1.5 mm的较浅缺陷,相位对比度相似,数据来自1个锁定期。

英文摘要:

Lock-In thermography is a useful Non Destructive Technique (NDT) for enhanced detection of defects in components, as it amplifies the phase contrast where defects exist. This amplification was found to be around 2-3 times compared to constant heating. The current used a Fuse Deposition Modelling (FDM) 3D printer to print samples with known defects, in order to characterise the relative effects of different variables on the Lock-In phase data. Samples were printed using ABS (Acrylonitrile Butadiene Styrene) and PLA (Polylactic Acid) for comparisons, and variables such as print direction, cameras, heating power, Lock-In frequency, as well as thickness, width and depth of defects were explored. It was found that different materials resulted in different baselines, but had similar phase contrast. A novel asynchronous technique was derived to enable Lock-In measurements with 5 different infrared cameras, and similar results were found. Even cheap cameras like the Seek Thermal CompactXR were proven capable of detecting the same defects as other cameras such as the FLIR SC7500. Heating power did not affect phase contrast, except for shallower defects up to 1.0 mm deep, where higher power resulted in better contrast. As expected, deeper defects could only be detected using lower Lock-In frequencies, and there was better phase contrast with wider, thicker and shallower defects. It was shown that defects 4 mm in width could be detected automatically up to a depth of around 1.5 mm, based on the phase signal trends. Sub-sampling of frame data showed that at least 10 frames were required per Lock-In period for minimal deviations in Lock-In phase contrast. Also, it was shown that phase contrast was similar for shallower defects up to 1.5 mm deep, with data from 1 Lock-In period, as long as the first frame was synchronised with the heating cycle.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑