高矫顽场$\varepsilon$ -Fe $_2$ O $_3$薄膜中的自旋Seebeck效应
Spin Seebeck effect in $\varepsilon$-Fe$_2$O$_3$ thin layer with high coercive field
摘要:
研究了Pt/ $\varepsilon$ -Fe $_2$ O $_3$双层膜的自旋Seebeck效应。采用旋涂法在Y:ZrO $_2$(100)衬底上制备了$40-70$ ~nm的$\varepsilon$ -Fe $_2$ O $_3$薄膜。所制备的层是高度取向的易磁化$a$ -轴平行于膜表面。在室温下,在平行于样品表面的磁场作用下测得的磁滞回线显示出高达11.6 kOe的矫顽场,这是迄今为止在$\varepsilon$ -Fe $_2$ O $_3$薄层样品中测得的最高值。自旋Seebeck磁滞回线的形状与矫顽场约为10 kOe的单相层的磁化强度的形状相似。在一些制备的层中,少量的二次软亚铁磁相揭示了由一个狭窄的形状的磁化循环,在相反的自旋塞贝克循环,没有收缩观察。在具有少量($1-2$ ~体积\%)次级软亚铁磁相的层的情况下遇到的差异,其通过磁化环的收缩形状揭示,与自旋塞贝克环相反,在自旋塞贝克环中没有观察到收缩。
英文摘要:
Spin Seebeck effect has been investigated in Pt/$\varepsilon$-Fe$_2$O$_3$ bilayers. The $\varepsilon$-Fe$_2$O$_3$ thin layer with $40-70$~nm thickness were deposited by a spin-coating method on Y:ZrO$_2$(100) substrates. The prepared layers are highly oriented with the easy magnetic $a$-axis parallel to the film surface. The magnetic hysteresis loops measured at room temperature with magnetic field parallel to the layer exhibit coercive fields up to 11.6~kOe, which is so far the highest value measured for $\varepsilon$-Fe$_2$O$_3$ thin layer samples. The shape of the spin Seebeck hysteresis loops is similar to the shape of magnetization for single phase layers with coercive field around 10~kOe. In some prepared layers a small amount of secondary soft ferrimagnetic phase is revealed by a constricted shape of magnetization loops, in contrast to spin Seebeck loops, where no constriction is observed. A difference in encountered in the case of layers with a small amount ($1-2$~volume\%) of secondary soft ferrimagnetic phase, which is revealed by a constricted shape of magnetization loops, in contrast to spin Seebeck loops, where no constriction is observed.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。