溶液喷吹纺丝法制备YBCO纳米陶瓷纤维
YBCO Ceramic Nanofibers obtained by the new technique of Solution Blow Spinning
摘要:
本研究提出一种新的溶液喷吹纺丝技术(SBS)制备YBCO陶瓷纳米纤维。前体溶液由Y、Ba和Cu金属乙酸盐(Ac)和聚(乙烯基吡咯烷酮)(PVP,Mw = 360,000)获得。测试了1:1和5:1的Ac:PVP浓度,分别产生平均直径为359和375 nm的陶瓷纳米纤维。X射线衍射证实了YBa_2Cu_3 O_(7-x)的纯相的形成。这是首次利用SBS制备YBCO纳米纤维,该技术有望获得高质量的陶瓷材料。
英文摘要:
This study proposes a novel solution blow spinning technique (SBS) for fabricating YBCO ceramic nanofibers. The precursor solutions were obtained from Y, Ba, and Cu metallic acetates (Ac) and poly(vinyl pyrrolidone) (PVP, Mw = 360,000). Ac:PVP concentrations of 1:1 and 5:1 were tested, resulting in ceramic nanofibers with average diameters of 359 and 375 nm, respectively. X-ray diffraction confirmed the formation of a pure phase of YBa2Cu3O7-x. This is the first study to use SBS for fabricating YBCO nanofibers, and this technique shows promise for obtaining high-quality ceramic materials.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。