氢等离子体处理的a-SiNx:H薄膜中的氢损及其改进的保留:使用100个MeV Ag7 +离子的ERDA研究

Hydrogen loss and its improved retention in hydrogen plasma treated a-SiNx:H films: ERDA study with 100 MeV Ag7+ ions

R. K. Bommali, S. Ghosh, S. A. Khan, P. Srivastava

摘要:

本文报道了用弹性反冲探测分析(ERDA)方法研究a-SiNx:H薄膜在100 MeV Ag ~(7+)离子辐照下的氢损。在分子复合模型的基本假设下解释了这些结果。ERDA氢计数由两个不同的氢解吸过程组成,在照射的初始阶段受到快速分子扩散的限制,并且随着能量密度的进展,受到原子氢扩散限制的缓慢过程接管。上述过程中的哪一个占主导地位,取决于膜内不断变化的氢浓度。ERDA测量也进行了低温(300摄氏度)氢等离子体退火(HPA)处理的薄膜。HPA处理的薄膜显示出改善的原子氢的扩散,导致愈合的弱键和钝化的悬挂键。此外,在HPA上,膜还显示出相对于沉积的膜,在先进的注量下具有显著更高的计数的氢的析出。这些结果表明HPA对a-SiNx:H膜中改善H保留的潜力。该研究清楚地区分了a-SiNx:H中两种扩散过程的存在,其扩散速率相差一个数量级,氢自由基不能从其产生点扩散超过约1 nm。研究结果对a-SiNx:H的钝化应用具有重要意义

英文摘要:

Hydrogen loss from a-SiNx:H films under irradiation with 100 MeV Ag7+ ions using elastic recoil detection analysis (ERDA) experiments is reported. The results are explained under the basic assumptions of the molecular recombination model. The ERDA hydrogen counts are composed of two distinct hydrogen desorption processes, limited by rapid molecular diffusion in the initial stages of irradiation, and as the fluence progresses a slow process limited by diffusion of atomic hydrogen takes over. Which of the aforesaid processes dominates, is determined by the continuously evolving Hydrogen concentration within the films. The ERDA measurements were also carried out for films treated with low temperature (300 degrees centigrade) hydrogen plasma annealing (HPA). The HPA treated films show an improved diffusion of atomic hydrogen, resulting from healing of weak bonds and passivation of dangling bonds. Further, upon HPA, films also show evolution of hydrogen with significantly higher counts, at advanced fluences, relative to the as-deposited films. These results indicate the potential of HPA towards improved H retention in a-SiNx:H films. The study distinguishes clearly the presence of two diffusion processes in a-SiNx:H whose diffusion rates differ by an order of magnitude, with hydrogen radicals not being able to diffuse beyond ~1 nm from the point of their creation. The results are very relevant for the passivation applications of a-SiNx:H

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑