通过高吸水性聚合物和丙纶纤维的组合在水泥材料中的自主修复:迈向可持续基础设施的一步

Autonomous Repair in Cementitous Material by Combination of Superabsorbent Polymers and Polypropylene Fibres: A Step Towards Sustainable Infrastructure

Souradeep Gupta, Harn Wei Kua, Sze Dai Pang

摘要:

混凝土结构裂缝的人工维护和修复往往是不可持续的,因为相关的劳动力,资金和环境的破坏。微纤维和高吸水性聚合物的引入是限制裂纹扩展和增强自愈合效率的材料解决方案。因此,该研究提出了聚丙烯(PP)纤维和高吸水性聚合物(SAP)的组合,这将有助于自主愈合和恢复原来的机械和耐久性性能的砂浆。愈合砂浆的机械强度,吸水性和水渗透性进行了比较,在相同的年龄,未损坏的砂浆,估计恢复原始性能,而裂缝密封通过光学显微镜进行了研究。实验结果表明,砂浆与PP纤维和SAP的组合显示出完全恢复愈合后的机械强度,而在耐久性恢复高达90%的记录。微观图像显示,在潮湿条件下,SAP和PP纤维的组合可以实现85%的平均裂缝密封率,而在干燥空气固化条件下的密封也显着高于仅用纤维的参考样品。裂缝宽度达330μm,已被碳酸盐晶体完全封闭。此外,具有SAP和PP纤维的砂浆在三次加载循环后保持其原始28天强度的约70%,而发现参考砂浆样品仅保持其原始强度的约40-50%。在含有SAP和纤维的砂浆中,有效的裂缝密封和原始性能的高恢复表明,这种材料组合将减少在使用寿命期间对环境破坏和昂贵维修的需求。

英文摘要:

Manual maintenance and repair of cracks in concrete structures are often unsustainable because of associated labor, capital and environmental damage. Introduction of microfibers and superabsorbent polymers is a material solution to restrict crack propagation and enhance self-healing efficiency. Therefore, the study proposes a combination of polypropylene(PP) fibers and superabsorbent polymers (SAP) which would facilitate autonomous healing and recover original mechanical and durability properties of mortar. Mechanical strength, sorptivity and water penetration of healed mortars were compared to that of undamaged mortar at same age to estimate recovery of original properties while crack sealing was investigated by means of optical microscopy. Experimental results show mortar with combination of PP fibers and SAP showed full recovery of mechanical strength after healing while recovery in durability up to 90% was recorded. Microscopic images show that average crack-sealing ratio of 85% could be achieved under moist condition by combination of SAP and PP fibers while sealing under drier air curing condition is also significantly higher than reference samples with only fibers. Crack width up to 330μm has been found to be completely sealed by carbonate crystals. Furthermore, mortar with SAP and PP fibers retain about 70% of their original 28-day strength after three cycles of loading while reference mortar samples were found to retain only about 40-50% of their original strength. Effective crack sealing and high recovery of original properties in mortars with SAP and fibers suggest that this material combination would reduce the need for environmentally damaging and expensive repairs during the service life.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑