Protocol to perform pressurized blister tests on thin elastic films
摘要:
这项工作的目的是确定常见的挑战,在准备的气泡测试装置设计用于测量脆性薄膜的能量释放率,并提出相应的易于实施的解决方案。为此,我们提供了一个分步指南,用于制造由粘附在玻璃基板上的聚苯乙烯薄膜组成的气泡测试装置。首先将薄膜从供体衬底转移到空气-水界面,然后将其用作平台以将它们定位在受体衬底上。我们在设备的背面嵌入了一个微通道,以排出被困在开口中的空气,通过开口施加压力。我们量化的高度和半径的水泡估计的粘附能量使用可用的表达式相关的法向力和时刻的形状的水泡。本起泡试验提供了聚苯乙烯在玻璃上的每单位面积$G = 18 \pm 2$ $ \mbox{mJ}/{\mbox m}^2$的粘附能,这与在我们的独立裂解试验中发现的$G = 14 \pm 2$ $ \mbox{mJ}/{\mbox m}^2$的测量结果非常一致。
英文摘要:
This work aims to identify common challenges in the preparation of the blister test devices designed for measurement of energy release rate for brittle thin films and to propose easy-to-implement solutions accordingly. To this end, we provide a step-by-step guide for fabricating a blister test device comprised of thin polystyrene films adhered to glass substrates. Thin films are first transferred from donor substrates to an air-water interface, which is then used as a platform to locate them on a receiver substrate. We embed a microchannel at the back of the device to evacuate the air trapped in the opening, through which the pressure is applied. We quantify the height and the radius of the blister to estimate the adhesion energy using the available expressions correlating the normal force and the moment with the shape of the blister. The present blister test provided adhesion energy per unit area of $G = 18 \pm 2$ $ \mbox{mJ}/{\mbox m}^2$ for polystyrene on glass, which is in good agreement with the measurement of $G = 14 \pm 2$ $ \mbox{mJ}/{\mbox m}^2$ found in our independent cleavage test.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。